Study on Preparation of Photocatalytic Material by Ce Doping in Titanium-Containing Blast Furnace Slag and Its Properties AITranslate
Abstract AITranslate
To achieve the comprehensive utilization of metallurgical solid waste titanium-containing blast furnace slag resources,the titanium-containing blast furnace slag(TiO2 mass fraction<20%)was used as the titanium source,and the Ce-doped titanium-containing blast furnace slag photocatalytic material was prepared by a high-temperature solid-phase doping method.The photocatalyst was characterized by XRD,SEM-EDS and UV-Vis DRS analytical techniques,and the effects of catalyst dosage,UV irradiation time and Rhodamine B(RhB)solution pH value on the photocatalytic performance of Ce-doped titanium-contai-ning blast furnace slag were investigated.The results show that Ce ions are successfully doped into the lat-tice of perovskite(CaTiO3)and diopside(CaO·MgO·2SiO2)by the high-temperature solid-phase do-ping method,and both CaTiO3 and CaO·MgO·2SiO2 participate in the photocatalytic degradation reac-tion of RhB solution.The addition of Ce ions enhances the light absorption capacity of titanium-containing blast-furnace slag and improves the efficiency of the catalyst in RhB degradation.Under the conditions of a catalyst dosage of 1.00 g,a irradiation time of 2.0 h,and a solution pH of 2,the degradation rate of 100 mL RhB solution with an initial concentration of 10 mg/L reaches 97.2%.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:O643.36[理学]
Citation Information:
To achieve the comprehensive utilization of metallurgical solid waste titanium-containing blast furnace slag resources,the titanium-containing blast furnace slag(TiO2 mass fraction<20%)was used as the titanium source,and the Ce-doped titanium-containing blast furnace slag photocatalytic material was prepared by a high-temperature solid-phase doping method.The photocatalyst was characterized by XRD,SEM-EDS and UV-Vis DRS analytical techniques,and the effects of catalyst dosage,UV irradiation time and Rhodamine B(RhB)solution pH value on the photocatalytic performance of Ce-doped titanium-contai-ning blast furnace slag were investigated.The results show that Ce ions are successfully doped into the lat-tice of perovskite(CaTiO3)and diopside(CaO·MgO·2SiO2)by the high-temperature solid-phase do-ping method,and both CaTiO3 and CaO·MgO·2SiO2 participate in the photocatalytic degradation reac-tion of RhB solution.The addition of Ce ions enhances the light absorption capacity of titanium-containing blast-furnace slag and improves the efficiency of the catalyst in RhB degradation.Under the conditions of a catalyst dosage of 1.00 g,a irradiation time of 2.0 h,and a solution pH of 2,the degradation rate of 100 mL RhB solution with an initial concentration of 10 mg/L reaches 97.2%.
quote
| GB/T 7714-2015 | [1] WANG Xin-bo, WANG Yang, ZHANG Ye, et al. Study on Preparation of Photocatalytic Material by Ce Doping in Titanium-Containing Blast Furnace Slag and Its Properties[J]. Rare Metals and Cemented Carbides, 2025(4): 58-65. |
| MLA | [1] WANG Xin-bo, et al., "Study on Preparation of Photocatalytic Material by Ce Doping in Titanium-Containing Blast Furnace Slag and Its Properties." Rare Metals and Cemented Carbides, no. 4, 2025, pp. 58-65. |
| APA | [1] WANG Xin-bo, WANG Yang, ZHANG Ye, TIAN Li, HUANG Guo-liang, XIE Jing, LIU Wen-yan, & ZHANG Li. (2025). Study on Preparation of Photocatalytic Material by Ce Doping in Titanium-Containing Blast Furnace Slag and Its Properties. Rare Metals and Cemented Carbides(4), 58-65. |
| IEEE | [1] WANG Xin-bo, WANG Yang, ZHANG Ye, TIAN Li, HUANG Guo-liang, XIE Jing, LIU Wen-yan, and ZHANG Li, "Study on Preparation of Photocatalytic Material by Ce Doping in Titanium-Containing Blast Furnace Slag and Its Properties," Rare Metals and Cemented Carbides, no. 4, pp. 58-65, 2025. keywords: {titanium-containing blast furnace slag;Ce doping;photocatalysis;high-temperature solid-phase} |