Influence assessment of new Inner Tube Porous Brick with absorbent concrete on urban floods control AITranslate

Chang’an University; Chang’an University; Wageningen University; Chang’an University; Guangdong Institute of Eco-environmental Science and Technology; University of California – Merced
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Super Absorbent Polymers enhanced the water absorption capacity of concrete. • The ITPB pavement has an apparent effect on reducing flood peak. • The ITPB pavement performs better for preventing long return period storms. • The ITPB pavement can infiltrate stormwater more efficient in clay area. As a part of low impact development (LID) measures, modifying the design of Inner Tube Porous Bricks (ITPB) may improve the functionality of the pavement to prevent urban floods. Absorbent concrete (AC) with different Super Absorbent Polymers (SAP) concentration was used as the brick materials to adsorb 311–376 l water per m3 AC after 120 min, and the hydraulic conductivity was calculated to vary between 34.59 mm/h and 74.8 mm/h for different ACs. The Storm Water Management Model (SWMM) is used here to simulate the influence of the ITPB on urban floods. When the return period (P) equals 100 years, the peak inflow of drainage networks can be decreased from 254.55 l/s to 91.12 l/s and the stormwater could be infiltrated 52.49 mm in low permeability areas (e.g. clay) by ITPB pavement. ITPB can be used as a new LID pavement in clay areas or be used to mitigate urban floods of long return period storms. Which should be noted is that the declared values about the simulation are valid in the study areas, further research is needed on the applicability of ITPB to the overall world. Graphical Download : Download high-res image (171KB) Download : Download full-size image

KeyWords AITranslate

Concrete New Inner Tube Porous Brick SWMM Super Absorbent Polymers Urban Flood Management
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2022.e01236

Chinese Library Classification Number:

Citation Information:

Highlights • Super Absorbent Polymers enhanced the water absorption capacity of concrete. • The ITPB pavement has an apparent effect on reducing flood peak. • The ITPB pavement performs better for preventing long return period storms. • The ITPB pavement can infiltrate stormwater more efficient in clay area. As a part of low impact development (LID) measures, modifying the design of Inner Tube Porous Bricks (ITPB) may improve the functionality of the pavement to prevent urban floods. Absorbent concrete (AC) with different Super Absorbent Polymers (SAP) concentration was used as the brick materials to adsorb 311–376 l water per m3 AC after 120 min, and the hydraulic conductivity was calculated to vary between 34.59 mm/h and 74.8 mm/h for different ACs. The Storm Water Management Model (SWMM) is used here to simulate the influence of the ITPB on urban floods. When the return period (P) equals 100 years, the peak inflow of drainage networks can be decreased from 254.55 l/s to 91.12 l/s and the stormwater could be infiltrated 52.49 mm in low permeability areas (e.g. clay) by ITPB pavement. ITPB can be used as a new LID pavement in clay areas or be used to mitigate urban floods of long return period storms. Which should be noted is that the declared values about the simulation are valid in the study areas, further research is needed on the applicability of ITPB to the overall world. Graphical Download : Download high-res image (171KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Pingping Luo, Liming Liu, Siting Wang, et al. Case Studies in Construction Materials, 2022(17). DOI:10.1016/j.cscm.2022.e01236.
MLA [1] Pingping Luo, et al., Case Studies in Construction Materials, no. 17, 2022, https://doi.org/10.1016/j.cscm.2022.e01236.
APA [1] Pingping Luo, Liming Liu, Siting Wang, Baiming Ren, Bin He, & Daniel Nover. (2022). Case Studies in Construction Materials(17). https://doi.org/10.1016/j.cscm.2022.e01236
IEEE [1] Pingping Luo, Liming Liu, Siting Wang, Baiming Ren, Bin He, and Daniel Nover, Case Studies in Construction Materials, no. 17, 2022, doi: 10.1016/j.cscm.2022.e01236. keywords: {Concrete;New Inner Tube Porous Brick;SWMM;Super Absorbent Polymers;Urban Flood Management}