Balancing Optical Property and Enhancing Stability for High-Refractive Index Polythiourethane with Assistance of Cubic Thiol-Functionalized Silsesquioxanes AITranslate
Abstract AITranslate
To achieve a better balance between the refractive index and Abbe number, the thiol-functionalized polyhedral oligomeric silsesquioxane (POSS–SH) was incorporated as both nanoreinforcement and cross-linking reagent into high-refractive index polythiourethane (PTU). The influences of the POSS–SH on the microstructures and properties of PTU were investigated. It is found that all the nanocomposites exhibited a dense network structure and high structural homogeneity even at the POSS–SH loading up to 10 wt %. Besides great improvements in the thermal stability and mechanical property, the nanocomposite containing 1.5 wt % POSS–SH revealed a slight reduction in the refractive index from 1.6568 for neat PTU to 1.6557 but a significant increase in the Abbe number from 28 to 35, accompanied by excellent optical transparency. These results indicate that the covalent incorporation of bifunctional POSS–SH into the PTU network will be helpful for the rational design of advanced optical and optoelectronic materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c00917
Chinese Library Classification Number:
Citation Information:
To achieve a better balance between the refractive index and Abbe number, the thiol-functionalized polyhedral oligomeric silsesquioxane (POSS–SH) was incorporated as both nanoreinforcement and cross-linking reagent into high-refractive index polythiourethane (PTU). The influences of the POSS–SH on the microstructures and properties of PTU were investigated. It is found that all the nanocomposites exhibited a dense network structure and high structural homogeneity even at the POSS–SH loading up to 10 wt %. Besides great improvements in the thermal stability and mechanical property, the nanocomposite containing 1.5 wt % POSS–SH revealed a slight reduction in the refractive index from 1.6568 for neat PTU to 1.6557 but a significant increase in the Abbe number from 28 to 35, accompanied by excellent optical transparency. These results indicate that the covalent incorporation of bifunctional POSS–SH into the PTU network will be helpful for the rational design of advanced optical and optoelectronic materials.
quote
| GB/T 7714-2015 | [1] Yuanyu Chen, Zongyi Qin, Guofeng Tang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c00917. |
| MLA | [1] Yuanyu Chen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c00917. |
| APA | [1] Yuanyu Chen, Zongyi Qin, Guofeng Tang, Lijun Wei, Houlin Du, & Weiping Du. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c00917 |
| IEEE | [1] Yuanyu Chen, Zongyi Qin, Guofeng Tang, Lijun Wei, Houlin Du, and Weiping Du, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c00917. keywords: {polythiourethane network;thiolfunctionalized POSS;nanocomposite;thermal stability;mechanical properties;optical properties} |