Characterization of Metal Cerium Film Prepared by Vacuum Vapor Deposition AITranslate
Abstract AITranslate
The metal cerium films were prepared on stainless steel substrate by vacuum vapor deposition.The morphology and phase structure of cerium films were investigated by scanning electron microscopy(SEM)and X-ray diffraction(XRD),and depth and chemical form of elements were measured by Auger electron spectroscopy(AES)and X-ray photoelectron spectroscopy(XPS).The results indicate that the surface of cerium film is compact and tightly bonded with stainless steel matrix,and its thickness is approximately 24μm.The surface of cerium film has been oxidized and the thickness of oxide film is about 340 nm,which is mainly composed of CeO2 and a small amount of Ce2O3.
KeyWords AITranslate
1戴春爱,刘博,颜鲁婷,刘莲云.铈作为环境材料的研究及应用[J].稀有金属材料与工程,2009,38(A01):357-360. 被引量:4
2林河成.金属铈的生产及应用[J].中国有色冶金,2005,34(3):31-34. 被引量:11
3罗立平,张赫.电磁感应加热蒸发金属铈及蒸气密度测量[J].稀有金属与硬质合金,2017,45(4):37-41. 被引量:2
4于震,孙亮,张志忠,张生栋,张晓卫.离子镀膜法制备铀薄膜的表征[J].核化学与放射化学,2014,36(5):277-281. 被引量:1
1张秀艳,常诚,包香春,张慧珍,于亚辉.硅藻土负载TODGA分离-电感耦合等离子体质谱法测定氧化铈中氧化钆、氧化铽[J].理化检验:化学分册,2021,57(7):642-647.
2张健,牛夏斌,孟辉波,齐振华,李建浩.探究氧气流量对新型高阻隔薄膜材料的制备及性能的影响[J].真空科学与技术学报,2021,41(7):694-698. 被引量:1
1张健,李建浩,齐振华,徐全国,唐智聪.直流磁控溅射对异形工件内表面沉积薄膜性能的影响[J].真空科学与技术学报,2022,42(3):223-227.
1张红州.电磁感应加热式道岔融雪系统方案研究[J].铁道通信信号,2019,55(8):34-36.
2赵佳龙,郑甲红,毛廷廷,霍启新,刘杰林.压光机电磁感应加热的实验研究[J].中国造纸,2019,38(8):63-67. 被引量:1
3陈星,张琦,汤彬,王海燕,姚启明,王健美,李睿,周冰科,林万明,李双寿.TiO2/x-GO纳米复合纤维的制备及其光催化性能的研究[J].太原理工大学学报,2019,50(5):562-567. 被引量:1
4鲁晓珂,李伟东,徐嫦松.古代白陶的元素分布及拉曼光谱分析[J].中国陶瓷,2019,55(8):66-77. 被引量:1
5张欣,巨东英,李建辉,张双杰,周达.溶胶-凝胶法制备铝合金耐蚀有机-无机杂化SiO2涂层及其性能研究[J].材料保护,2019,0(7):12-16. 被引量:5
6朱萌萌,李国华,张雪明,翟佳欣,甘思平,宋潇.氮化硼纳米片负载纳米Cu2O及其催化还原对硝基苯酚[J].无机材料学报,2019,34(8):817-826. 被引量:1
7任逸,施梦琦,尹越,张炜铭,吕路,柏益尧.Fe_(2)O_(3)/MIL-53(Al)催化类芬顿氧化性能及其作用机制研究[J].环境科学学报,2019,39(8):2508-2516. 被引量:7
8徐杰,陈新,王玲玲.用过期切片面包制备环保超级电容器活性炭电极材料[J].化工学报,2019,70(9):3582-3589. 被引量:5
9李翠霞,康伟超,任一波,王慧康,史晓.介孔TiO2/rGO交替薄膜光催化降解土霉素[J].兰州理工大学学报,2019,45(4):6-10. 被引量:1
10陈文书,顾佳俊.单层二硫化钼的电化学嵌锂及液相剥离制备工艺研究[J].冶金与材料,2019,39(4):9-10. 被引量:6
Basic Information:
DOI:
Chinese Library Classification Number:TG174.444[金属学及工艺—金属表面处理]
Citation Information:
The metal cerium films were prepared on stainless steel substrate by vacuum vapor deposition.The morphology and phase structure of cerium films were investigated by scanning electron microscopy(SEM)and X-ray diffraction(XRD),and depth and chemical form of elements were measured by Auger electron spectroscopy(AES)and X-ray photoelectron spectroscopy(XPS).The results indicate that the surface of cerium film is compact and tightly bonded with stainless steel matrix,and its thickness is approximately 24μm.The surface of cerium film has been oxidized and the thickness of oxide film is about 340 nm,which is mainly composed of CeO2 and a small amount of Ce2O3.
quote
| GB/T 7714-2015 | [1] LV Xu-ming, MA Xian, HE Ying, et al. Characterization of Metal Cerium Film Prepared by Vacuum Vapor Deposition[J]. Rare Metals and Cemented Carbides, 2019(4): 39-43. |
| MLA | [1] LV Xu-ming, et al., "Characterization of Metal Cerium Film Prepared by Vacuum Vapor Deposition." Rare Metals and Cemented Carbides, no. 4, 2019, pp. 39-43. |
| APA | [1] LV Xu-ming, MA Xian, HE Ying, LUO Li-ping, & ZHANG Xiao-wei. (2019). Characterization of Metal Cerium Film Prepared by Vacuum Vapor Deposition. Rare Metals and Cemented Carbides(4), 39-43. |
| IEEE | [1] LV Xu-ming, MA Xian, HE Ying, LUO Li-ping, and ZHANG Xiao-wei, "Characterization of Metal Cerium Film Prepared by Vacuum Vapor Deposition," Rare Metals and Cemented Carbides, no. 4, pp. 39-43, 2019. keywords: {vacuum vapor deposition;electromagnetic induction heating;cerium film;stainless steel substrate} |