daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Effect of Halogenation Agents on Preparation of Nano VC Whiskers AITranslate

Department of Materials Science and Engineering,Sichuan University of Science and Engineering;Department of Materials Science and Engineering,Sichuan University of Science and Engineering;Department of Materials Science and Engineering,Sichuan University of Science and Engineering;Department of Materials Science and Engineering,Sichuan University of Science and Engineering;Department of Materials Science and Engineering,Sichuan University of Science and Engineering;Department of Materials Science and Engineering,Sichuan University of Science and Engineering
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nano VC whiskers were prepared by using ammonium metavanadate,xylose,etc.as precursor materials with carbothermal reduction method.The effects of type and dosage of halogenation agents on the preparation of nano VC whiskers were studied by SEM,TEM and XRD.The results show that nano VC whiskers with about 100 nm diameter,smooth surface and good morphology can be prepared at 1000℃for 2 h by adding 10%NaF as the halogenation agent.NaF is the most ideal halogenation agent for preparing VC whiskers in six kinds of halogenation agents.The dosage of halogenation agents has an important influence on the preparation of nano VC whiskers.The optimal dosage of NaF is 10%.Too little NaF cannot promote the growth of VC whiskers,while too much NaF will inhibit the growth of VC whiskers.

KeyWords AITranslate

nano VC whisker precursor carbothermal reduction halogenation agent type dosage

1曹冲,周涛,李文魁,艾建平.自蔓延燃烧合成氮化铝晶须及其生长机理[J].江西科技师范大学学报,2017,12(6):13-16. 被引量:2

2康浩,潘文平.纳米碳化钒的制备及其表征分析[J].陶瓷,2018(9):52-58. 被引量:2

3蒋小朗,金永中,马世卿,周锐,郑婷.前驱体法制备纳米VC晶须的研究[J].稀有金属与硬质合金,2020(1):51-55. 被引量:1

4杜炜,艾超前,马雪东,杜毅帆,王伟.无机晶须的制备及应用进展[J].应用化工,2019,48(5):1163-1166. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]

Citation Information:

Nano VC whiskers were prepared by using ammonium metavanadate,xylose,etc.as precursor materials with carbothermal reduction method.The effects of type and dosage of halogenation agents on the preparation of nano VC whiskers were studied by SEM,TEM and XRD.The results show that nano VC whiskers with about 100 nm diameter,smooth surface and good morphology can be prepared at 1000℃for 2 h by adding 10%NaF as the halogenation agent.NaF is the most ideal halogenation agent for preparing VC whiskers in six kinds of halogenation agents.The dosage of halogenation agents has an important influence on the preparation of nano VC whiskers.The optimal dosage of NaF is 10%.Too little NaF cannot promote the growth of VC whiskers,while too much NaF will inhibit the growth of VC whiskers.

quote

GB/T 7714-2015 [1] ZHOU Rui, JIN Yong-zhong, MA Shi-qing, et al. Effect of Halogenation Agents on Preparation of Nano VC Whiskers[J]. Rare Metals and Cemented Carbides, 2021(1): 52-56.
MLA [1] ZHOU Rui, et al., "Effect of Halogenation Agents on Preparation of Nano VC Whiskers." Rare Metals and Cemented Carbides, no. 1, 2021, pp. 52-56.
APA [1] ZHOU Rui, JIN Yong-zhong, MA Shi-qing, JIANG Xiao-lang, FANG Yong, & TANG Zhang-heng. (2021). Effect of Halogenation Agents on Preparation of Nano VC Whiskers. Rare Metals and Cemented Carbides(1), 52-56.
IEEE [1] ZHOU Rui, JIN Yong-zhong, MA Shi-qing, JIANG Xiao-lang, FANG Yong, and TANG Zhang-heng, "Effect of Halogenation Agents on Preparation of Nano VC Whiskers," Rare Metals and Cemented Carbides, no. 1, pp. 52-56, 2021. keywords: {nano VC whisker;precursor;carbothermal reduction;halogenation agent;type;dosage}