daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Polymer Bridging Induced by a Single Additive Imparts Easy-To-Implement Green Machinability to Yttria-Stabilized Zirconia AITranslate

Sabanci University; Sabanci University; Sabanci University; Sabanci University; Sabanci University; Sabanci University; University College London; Sabanci University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cold isostatic pressing, gelcasting, and protein coagulation are the main methods to produce machinable green bodies of ceramics. They generally employ multiple additives, such as binders, dispersants, and coagulants, and require numerous steps to embody a green body that can withstand further shaping and machining. This study reports a method that forms a ceramic dough that can be manipulated by hand, cut, or pushed into a mold. This facile method relies on a single additive─a linear copolymer─to homogeneously coagulate yttria-stabilized zirconia through polymer bridging. The structure of the additive is systematically designed, and the amount to be used in the formulations is optimized through electrokinetic and rheological studies. The use of this additive at 1 wt % generates ceramic objects with ∼22% shrinkage and a density of 5.95 ± 0.02 g cm–3 after sintering and enables the fabrication of intricate shapes such as structures with triangle and hexagonal cavities via laser cutting and holes in high aspect ratio objects via conventional machining.

KeyWords AITranslate

green body rapid prototyping machining of ceramics processing of ceramics additives
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00605

Chinese Library Classification Number:

Citation Information:

Cold isostatic pressing, gelcasting, and protein coagulation are the main methods to produce machinable green bodies of ceramics. They generally employ multiple additives, such as binders, dispersants, and coagulants, and require numerous steps to embody a green body that can withstand further shaping and machining. This study reports a method that forms a ceramic dough that can be manipulated by hand, cut, or pushed into a mold. This facile method relies on a single additive─a linear copolymer─to homogeneously coagulate yttria-stabilized zirconia through polymer bridging. The structure of the additive is systematically designed, and the amount to be used in the formulations is optimized through electrokinetic and rheological studies. The use of this additive at 1 wt % generates ceramic objects with ∼22% shrinkage and a density of 5.95 ± 0.02 g cm–3 after sintering and enables the fabrication of intricate shapes such as structures with triangle and hexagonal cavities via laser cutting and holes in high aspect ratio objects via conventional machining.

quote

GB/T 7714-2015 [1] Lyn Zemberekci, Gizem Demir, Can Akaoglu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00605.
MLA [1] Lyn Zemberekci, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00605.
APA [1] Lyn Zemberekci, Gizem Demir, Can Akaoglu, Wael Ali Aldulaimi, Aleyna Beste Ozhan, Mehmet Ali Gulgun, Omid Akhlaghi, & Ozge Akbulut. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00605
IEEE [1] Lyn Zemberekci, Gizem Demir, Can Akaoglu, Wael Ali Aldulaimi, Aleyna Beste Ozhan, Mehmet Ali Gulgun, Omid Akhlaghi, and Ozge Akbulut, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00605. keywords: {green body;rapid prototyping;machining of ceramics;processing of ceramics;additives}