The Latest Development of Research and Application on Electroless Crystal Co-P Alloy AITranslate

College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology;College of Materials Science and Engineering, Hefei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The deposition mechanism, microstructure and comprehensive properties of eletroless crystal Co-P alloy are described, and its industrial application is introduced in detail. Furthermore, its existing problems and development trend are pointed out.

KeyWords AITranslate

electroless plating crystal Co-P alloy deposition mechanism comprehensive property industrial application development trend

1张积桥,杨玉国,朱红,王芳辉.碳纤维化学镀钴工艺研究[J].电镀与精饰,2008,30(5):33-35. 被引量:5

2高诚辉,柳丽娜,林有希,李友遐.化学镀非晶态合金磁性的控制[J].电镀与环保,2003,23(5):22-26. 被引量:4

3李宁,何世禹,申日辉,李铭华,陈玲.耐热疲劳性镀层的研究[J].材料保护,1994,27(11):13-15. 被引量:3

4曾鹏,郑国桢,王德芳,黄拿灿,胡社军,王桂棠.化学镀Co-P合金镀层的非晶结构条件及性能研究[J].材料保护,1999,32(12):4-5. 被引量:10

5宣天鹏,郑晓华,刘玉,邓宗钢.操作条件对化学镀Co-P薄膜磁性的影响[J].材料保护,1998,31(5):12-13. 被引量:10

6张慧泽,刘涛,王幼文,凌国平,郦剑.氮化硅超细粉钴磷合金镀层的制备[J].中国有色金属学报,2003,13(3):713-716. 被引量:11

7孙宏飞,葛圣松,万殿茂,刘继林,陈学宁.非晶态镍磷合金层附着强度的研究[J].山东科学,1997,10(4):44-47. 被引量:3

8田永毅,李明.石墨与碳纳米管的化学镀Co—P合金[J].重庆工业高等专科学校学报,2004,19(5):5-6. 被引量:7

9朱绍峰,邓宗钢.化学镀钴磷合金的特性[J].表面技术,1992,21(6):266-269. 被引量:5

10时刻,黄英,廖梓珺,祖恩峰,张龙彬,王利.玻璃纤维化学镀Co-P合金工艺研究[J].材料保护,2005,38(6):27-29. 被引量:8

1张焱,陈丽娜,尤显卿,杨庆海.钴磷合金镀层的热疲劳组织结构变化的研究[J].兵器材料科学与工程,2011,34(1):41-44.

2胡勇涛,李玉龙,茶映鹏.光纤布拉格光栅化学镀钴层的温度传感性能[J].材料保护,2014,47(7):38-41. 被引量:2

3谭俊,宋皓.电流密度对喷射电沉积钴–磷合金镀层的影响[J].电镀与涂饰,2017,36(1):12-15. 被引量:1

4宋皓,谭俊,郑晓辉,张庆,王猛,张啸宇,阳振宇.Co-P合金镀层的研究现状[J].表面技术,2017,46(8):102-108. 被引量:1

5许友,方志刚,廖薇,秦渝.团簇Co4P的热力学稳定性及电子性质[J].内蒙古师范大学学报:自然科学汉文版,2020,49(4):353-359.

1张常兴,黄浩,黄璐瑶,陈小华,黄露,马素德.高紫外光透过率光纤涂料的制备[J].化工新型材料,2020,48(5):117-119.

2唐春华.现代镀覆技术 第五部分——其他化学镀[J].电镀与涂饰,2021,40(9):691-695.

3单凤君,王双红.工艺参数对锌镍合金镀层组织及性能的影响[J].电镀与涂饰,2021,40(11):829-833. 被引量:1

4李敏,张胜健,曹秋菊.桐油覆膜Ni-Co-SiO2纳米复合涂层的制备及防腐性能研究[J].电镀与精饰,2023,45(1):8-15.

1严怡芹,倪光明.微量铈离子在酸性电镀锡过程中沉积机理的探讨[J].安徽师大学报,1994,17(4):46-51.

2孙建春,王健,彭晓东.纳米复合镀层的沉积机理及其摩擦特性的研究现状[J].材料导报,2003,17(4):61-62. 被引量:16

3沈风雷,王红卫,闻荻江.电解有机溶液法制备类金刚石薄膜[J].苏州大学学报:工科版,2003,23(4):38-43.

4费维栋,李超,刘宗荣.金属玻璃的晶化[J].兵器材料科学与工程,1990(11):52-59.

5张英杰,董鹏,范云鹰.Zn-Ni合金镀层沉积机理及腐蚀机理研究进展[J].材料保护,2007,40(11):45-48. 被引量:5

6李觅.圣戈班玻璃俱乐部之谜[J].建材与装饰,2006(11):22-23.

7杜继红,李争显,刘素英,周慧,黄春良.钛合金镀银工艺的研究[J].有色冶炼,2002,31(6):186-186. 被引量:1

8杜继红,李争显,刘素英,周慧,黄春良.钛合金镀银工艺的研究[J].表面技术,2002,31(5):40-41. 被引量:2

9李文献.定窑纹饰组织结构简析[J].河北陶瓷,1991(3):37-40.

10魏涛,周玉,雷廷权.自生α/β-Sialon复相陶瓷的组织结构及形成机制[J].材料科学与工艺,1997,5(1):99-102. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ153.2[化学工程—电化学工业]

Citation Information:

The deposition mechanism, microstructure and comprehensive properties of eletroless crystal Co-P alloy are described, and its industrial application is introduced in detail. Furthermore, its existing problems and development trend are pointed out.

quote

GB/T 7714-2015 [1] YANG Qing-hai, YOU Xian-qing, ZHANG Yan, et al. The Latest Development of Research and Application on Electroless Crystal Co-P Alloy[J]. Rare Metals and Cemented Carbides, 2009(2): 58-62.
MLA [1] YANG Qing-hai, et al., "The Latest Development of Research and Application on Electroless Crystal Co-P Alloy." Rare Metals and Cemented Carbides, no. 2, 2009, pp. 58-62.
APA [1] YANG Qing-hai, YOU Xian-qing, ZHANG Yan, & CHEN Li-na. (2009). The Latest Development of Research and Application on Electroless Crystal Co-P Alloy. Rare Metals and Cemented Carbides(2), 58-62.
IEEE [1] YANG Qing-hai, YOU Xian-qing, ZHANG Yan, and CHEN Li-na, "The Latest Development of Research and Application on Electroless Crystal Co-P Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 58-62, 2009. keywords: {electroless plating;crystal Co-P alloy;deposition mechanism;comprehensive property;industrial application;development trend}