Coordination Mode-Regulated Lanthanide Supramolecular Hydrogels with Tunable Luminescence and Stimuli-Responsive Properties AITranslate
Abstract AITranslate
Hydrogels with tunable luminescence and stimuli responsiveness have attracted wide interest, owing to the desire to design soft machines and/or wearable electronic devices. Yet, it is challenging to obtain those that possess multicolorimetric change properties when exposed to complex mechanical stimuli and are strong, elastic, and capable of self-healing. Strong polymers with adjustable and switchable mechanical and fluorescence properties were designed using fluorescent lanthanide (Eu/Tb) as a cross-linker. The resulting compounds contained dynamic coordination and hydrogen bonds forming the physical cross-linking network; sodium 4-(allyloxy)pyridine-2,6-dicarboxylate (SPD) and H2O ligands coordinated with Eu/Tb(III) centers through different coordination modes and interactions. Three SPDs coordinated with Tb(III), and two SPDs and three weaker H2O coordinated with Eu(III). As a result, Eu/Tb–ligand bonds with different degrees of cleavages showed changes in the fluorescence color when exposed to complex mechanical stimuli. Also, for the reversible formation and dissociation of the Eu/Tb–SPD complexes, the designed hydrogel showed potential application in human fingerprint sensing.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00542
Chinese Library Classification Number:
Citation Information:
Hydrogels with tunable luminescence and stimuli responsiveness have attracted wide interest, owing to the desire to design soft machines and/or wearable electronic devices. Yet, it is challenging to obtain those that possess multicolorimetric change properties when exposed to complex mechanical stimuli and are strong, elastic, and capable of self-healing. Strong polymers with adjustable and switchable mechanical and fluorescence properties were designed using fluorescent lanthanide (Eu/Tb) as a cross-linker. The resulting compounds contained dynamic coordination and hydrogen bonds forming the physical cross-linking network; sodium 4-(allyloxy)pyridine-2,6-dicarboxylate (SPD) and H2O ligands coordinated with Eu/Tb(III) centers through different coordination modes and interactions. Three SPDs coordinated with Tb(III), and two SPDs and three weaker H2O coordinated with Eu(III). As a result, Eu/Tb–ligand bonds with different degrees of cleavages showed changes in the fluorescence color when exposed to complex mechanical stimuli. Also, for the reversible formation and dissociation of the Eu/Tb–SPD complexes, the designed hydrogel showed potential application in human fingerprint sensing.
quote
| GB/T 7714-2015 | [1] Longyue Yu, Ruiguang Zhao, Ning Wang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00542. |
| MLA | [1] Longyue Yu, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00542. |
| APA | [1] Longyue Yu, Ruiguang Zhao, Ning Wang, Shengyu Feng, & XingDong Xu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00542 |