Near-Infrared Light Induced Dynamic Structural Color Change of Amorphous Photonic Hydrogel AITranslate
Abstract AITranslate
Light-induced photonic systems are rare in nature and usually lack a full color response in artificial systems. Herein, we first report a near-infrared (NIR) light controlled optical hydrogel; its structural color covers the full visible spectrum range. The hydrogel was fabricated by embedding dry thermoresponsive microgels film into a thermoresponsive hydrogel. Under the synergistic effect of the microgels and hydrogel, the hydrogel displayed a dynamic color with temperature changing, and it was reversible. Moreover, the structural colors were angle independent for the amorphous microgel arrays. When carbon nanotubes were integrated into the matrix hydrogel, dynamic structural colors can be displayed under NIR irradiation. Such NIR light-responsive photonic hydrogel film may provide potential applications in artificial skin, the military, and other fields.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01045
Chinese Library Classification Number:
Citation Information:
Light-induced photonic systems are rare in nature and usually lack a full color response in artificial systems. Herein, we first report a near-infrared (NIR) light controlled optical hydrogel; its structural color covers the full visible spectrum range. The hydrogel was fabricated by embedding dry thermoresponsive microgels film into a thermoresponsive hydrogel. Under the synergistic effect of the microgels and hydrogel, the hydrogel displayed a dynamic color with temperature changing, and it was reversible. Moreover, the structural colors were angle independent for the amorphous microgel arrays. When carbon nanotubes were integrated into the matrix hydrogel, dynamic structural colors can be displayed under NIR irradiation. Such NIR light-responsive photonic hydrogel film may provide potential applications in artificial skin, the military, and other fields.
quote
| GB/T 7714-2015 | [1] Yongqing Xia, Shuai Gao, Ronghua Yu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01045. |
| MLA | [1] Yongqing Xia, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01045. |
| APA | [1] Yongqing Xia, Shuai Gao, Ronghua Yu, Zhujun Zeng, Hua He, Xiaohan Zhou, Ying Hu, Meiwen Cao, & Shengjie Wang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01045 |
| IEEE | [1] Yongqing Xia, Shuai Gao, Ronghua Yu, Zhujun Zeng, Hua He, Xiaohan Zhou, Ying Hu, Meiwen Cao, and Shengjie Wang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01045. keywords: {NIR responsive;optical hydrogel;thermoresponsive microgel;angle independent;carbon nanotubes} |