Bio-Based Flame Retardation of Acrylonitrile–Butadiene–Styrene AITranslate
Abstract AITranslate
Bio-based flame retardants (FRs) were employed to successfully reduce the flammability of acrylonitrile–butadiene–styrene (ABS), achieving results comparable to a commercial brominated ABS product (Br-ABS); synergistic interactions between the components were responsible for the enhanced performance. In a two-phase study, eight nonhalogenated, low-toxicity FRs and combinations thereof were melt-processed with ABS at a 30 wt % FR content and screened using microscale combustion calorimetry (MCC). All 30 samples presented significantly lower peak heat release rates (PHRR; 26–43% reduction) and total heat release (THR; 16–29% reduction) than ABS. Four best-performing compositions─ABS/tannic acid (TA), ABS/tannic acid/fish gelatin (TA-FG), ABS/phytic acid sodium salt (PA), and ABS/phytic acid sodium salt/tannic acid (PA-TA)─were scaled up and further analyzed through cone calorimetry (CC) and mechanical testing. TA, TA-FG, PA, and PA-TA significantly lowered ABS’s PHRR in MCC (36–43% reduction) and in CC (38–65% reduction). Some samples matched commercial brominated ABS: TA in MCC and PA-TA in CC. The mechanical performances of the composites were acceptable, with an increase in modulus but a loss in toughness. Important synergistic interactions between the FRs and the ABS matrix, between TA and FG, and between PA and TA, were responsible for the reduced flammabilities.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01155
Chinese Library Classification Number:
Citation Information:
Bio-based flame retardants (FRs) were employed to successfully reduce the flammability of acrylonitrile–butadiene–styrene (ABS), achieving results comparable to a commercial brominated ABS product (Br-ABS); synergistic interactions between the components were responsible for the enhanced performance. In a two-phase study, eight nonhalogenated, low-toxicity FRs and combinations thereof were melt-processed with ABS at a 30 wt % FR content and screened using microscale combustion calorimetry (MCC). All 30 samples presented significantly lower peak heat release rates (PHRR; 26–43% reduction) and total heat release (THR; 16–29% reduction) than ABS. Four best-performing compositions─ABS/tannic acid (TA), ABS/tannic acid/fish gelatin (TA-FG), ABS/phytic acid sodium salt (PA), and ABS/phytic acid sodium salt/tannic acid (PA-TA)─were scaled up and further analyzed through cone calorimetry (CC) and mechanical testing. TA, TA-FG, PA, and PA-TA significantly lowered ABS’s PHRR in MCC (36–43% reduction) and in CC (38–65% reduction). Some samples matched commercial brominated ABS: TA in MCC and PA-TA in CC. The mechanical performances of the composites were acceptable, with an increase in modulus but a loss in toughness. Important synergistic interactions between the FRs and the ABS matrix, between TA and FG, and between PA and TA, were responsible for the reduced flammabilities.
quote
| GB/T 7714-2015 | [1] Gustavo Schinazi, José Roberto Moraes d’Almeida, Jonathan K. Pokorski, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01155. |
| MLA | [1] Gustavo Schinazi, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01155. |
| APA | [1] Gustavo Schinazi, José Roberto Moraes d’Almeida, Jonathan K. Pokorski, & David A. Schiraldi. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01155 |
| IEEE | [1] Gustavo Schinazi, José Roberto Moraes d’Almeida, Jonathan K. Pokorski, and David A. Schiraldi, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01155. keywords: {flammability;ABS;biobased;bromine;flame retardant;calorimetry;tannic acid;phytic acid} |