Twinning and Texture Evolution of Beryllium during Room Temperature Deformation AITranslate

State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Materials Research Institute Ningxia Co.,Ltd.;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Materials Research Institute Ningxia Co.,Ltd.;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Materials Research Institute Ningxia Co.,Ltd.;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Materials Research Institute Ningxia Co.,Ltd.;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Materials Research Institute Ningxia Co.,Ltd.;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Materials Research Institute Ningxia Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The universal testing machine was used to carry out different strain compression tests of the isostatic-pressure beryllium at room temperature.SEM and EBSD were used to analysis twinning formation and texture evolution in beryllium material. The results show that only stretching twinning {1012} of be ryllium forms during room temperature compression. During the evolution of stretched twinning,twinning formation and growth has great promotion effect on the large-angle changing of grains and the formation of new texture {0001}. However,the coordination effect is reduced on the slip deformation of beryllium dur ing the later twinning period. In addition, uniaxial compression couples also play an important role in the formation of new texture {0001}.

KeyWords AITranslate

beryllium stretched twinning slip texture

1宋德军,张习敏,胡强,周成.铍焊接技术研究发展概况[J].材料导报,2006,20(2):66-69. 被引量:8

2代彦明,王东新,张健康,吕一格,李美岁,李军义,李少银,钟景明.不同应变速率下铍材的拉伸性能及变形行为[J].稀有金属与硬质合金,2018,46(2):54-58. 被引量:2

3王长义,刘正,毛萍莉.{102}拉伸孪晶对AZ31B镁合金动态力学行为及应变速率敏感性的影响[J].热加工工艺,2011,40(12):19-21. 被引量:7

1郑莉芳,刘新宇,鲍帅平,张健康,钟景明,丁玉龙.稀有金属铍的性能研究进展[J].稀有金属,2023,47(2):292-302.

1唐昌平,成声亮,李国栋.Mg-Gd-Y-Nd-Zr合金热变形过程中的组织与织构演变[J].材料科学,2016,6(5):292-299.

2孙明帅,宁江利,李杰,赵重阳,冯运莉.热轧态AZ31B镁合金单向拉伸塑性变形机制研究[J].轻合金加工技术,2019,47(2):33-37. 被引量:1

3付盼,廖明豪,田中兰,李军,乔磊,李林,吴志勇.页岩气水平井压裂中地层滑移数值模拟研究[J].石油机械,2019,47(4):73-79. 被引量:12

4徐春,饶小华,安星州,陈雪,朱文峰.轧制方式对工业纯钛TA2轧板织构演变的影响[J].稀有金属材料与工程,2019,48(4):1195-1201. 被引量:4

5张晶晶(编译).稳定化的高锯铁素体不锈钢在多道次热变形中的微结构和织构演变[J].不锈,2019,0(1):4-14.

6郑国明,李磊,毛小南,蔡建华,吴聪,雷磊.钛合金BCC?HCP相变的变体选择及其对晶体取向的影响[J].材料导报,2019,33(17):2910-2917. 被引量:4

7陈亮维,霍广鹏,虞澜,胡劲.金属锆织构的标准极图计算及分析[J].昆明理工大学学报:自然科学版,2019,44(2):19-25. 被引量:5

8李嫚,王帅康,程职玲,张弘弢.基于ABAQUS的镍基高温合金锯齿形切屑演变过程及机理研究[J].工具技术,2019,53(1):36-42. 被引量:2

9党宁,刘玲玉,LAVOGIEZ Cyril,MAIRE Eric,马朝利,周廉.激光焊接Ti-6Al-4V钛合金塑性行为的原位SEM/EBSD分析(英文)[J].中国材料进展,2019,38(3):279-285.

10刘后龙,马明玉,刘玲玲,魏亮亮,陈礼清.热轧板退火工艺对19Cr2Mo1W铁素体不锈钢织构与成形性能的影响[J].金属学报,2019,55(5):566-574. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TG146.24[金属学及工艺—金属材料]

Citation Information:

The universal testing machine was used to carry out different strain compression tests of the isostatic-pressure beryllium at room temperature.SEM and EBSD were used to analysis twinning formation and texture evolution in beryllium material. The results show that only stretching twinning {1012} of be ryllium forms during room temperature compression. During the evolution of stretched twinning,twinning formation and growth has great promotion effect on the large-angle changing of grains and the formation of new texture {0001}. However,the coordination effect is reduced on the slip deformation of beryllium dur ing the later twinning period. In addition, uniaxial compression couples also play an important role in the formation of new texture {0001}.

quote

GB/T 7714-2015 [1] DAI Yan-ming, LV Yi-ge, WANG Dong-xin, et al. Twinning and Texture Evolution of Beryllium during Room Temperature Deformation[J]. Rare Metals and Cemented Carbides, 2019(3): 42-46.
MLA [1] DAI Yan-ming, et al., "Twinning and Texture Evolution of Beryllium during Room Temperature Deformation." Rare Metals and Cemented Carbides, no. 3, 2019, pp. 42-46.
APA [1] DAI Yan-ming, LV Yi-ge, WANG Dong-xin, ZHANG Jian-kang, XU De-mei, & ZHONG Jing-ming. (2019). Twinning and Texture Evolution of Beryllium during Room Temperature Deformation. Rare Metals and Cemented Carbides(3), 42-46.
IEEE [1] DAI Yan-ming, LV Yi-ge, WANG Dong-xin, ZHANG Jian-kang, XU De-mei, and ZHONG Jing-ming, "Twinning and Texture Evolution of Beryllium during Room Temperature Deformation," Rare Metals and Cemented Carbides, no. 3, pp. 42-46, 2019. keywords: {beryllium;stretched twinning;slip;texture}