Organic–inorganic two-dimensional (2D) perovskite is an optoelectronic material, with quantum-well structure and improved moisture stabilities, which has been widely used in various optoelectronic devices recently. In this review, the structure and properties of organic–inorganic 2D perovskite materials are first briefly introduced. After that, according to the different photoelectron coupling mechanisms, the recent progress of typical 2D perovskite-based optoelectronic devices is described in detail: including photodetectors, light-emitting diodes, solar cells, and lasers, as well as some optoelectronic devices (e.g., optical memory and optical synapses). We analyzed the influence of structure, manufacturing process, and material selection on device performance and showed promising progress in different applications. Subsequently, we proposed the possible breakthrough development direction of 2D perovskite-based optoelectronic devices in the coming years. This work points out the way for future progress of 2D perovskite-based optoelectronic devices, which is conducive to further improving device performance and inspiring designs of high-performance organic–inorganic 2D perovskite-based optoelectronic devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c00781
Chinese Library Classification Number:
Citation Information:
Organic–inorganic two-dimensional (2D) perovskite is an optoelectronic material, with quantum-well structure and improved moisture stabilities, which has been widely used in various optoelectronic devices recently. In this review, the structure and properties of organic–inorganic 2D perovskite materials are first briefly introduced. After that, according to the different photoelectron coupling mechanisms, the recent progress of typical 2D perovskite-based optoelectronic devices is described in detail: including photodetectors, light-emitting diodes, solar cells, and lasers, as well as some optoelectronic devices (e.g., optical memory and optical synapses). We analyzed the influence of structure, manufacturing process, and material selection on device performance and showed promising progress in different applications. Subsequently, we proposed the possible breakthrough development direction of 2D perovskite-based optoelectronic devices in the coming years. This work points out the way for future progress of 2D perovskite-based optoelectronic devices, which is conducive to further improving device performance and inspiring designs of high-performance organic–inorganic 2D perovskite-based optoelectronic devices.
quote
| GB/T 7714-2015 | [1] YuTao Li, Lei Han, Hang Liu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c00781. |
| MLA | [1] YuTao Li, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c00781. |
| APA | [1] YuTao Li, Lei Han, Hang Liu, Kuan Sun, Di Luo, XiaoLiang Guo, DuLi Yu, & TianLing Ren. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c00781 |
| IEEE | [1] YuTao Li, Lei Han, Hang Liu, Kuan Sun, Di Luo, XiaoLiang Guo, DuLi Yu, and TianLing Ren, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c00781. keywords: {twodimensional perovskite solar cell photodetector LED laser material composite} |