daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Ultrafast Photo-Crosslinking of Thiol–Norbornene Opaque Silicone Elastomer Nanocomposites in Air AITranslate

Queen Mary University of London; Queen Mary University of London; Queen Mary University of London; Queen Mary University of London; Queen Mary University of London
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Photocured silicone elastomers have become increasingly popular in a variety of advanced materials applications including soft robotics, biomedical devices, microfabrication, functional coatings, and additive manufacturing. Oxygen inhibition, however, remains a major challenge for conventional photoradical curing, limiting applications and restricting processing. Here, we report a thiol–norbornene-based silicone system using a polydimethylsiloxane (PDMS) displaying terminal norbornene groups and a highly functionalized thiolated PDMS to achieve very fast curing speeds in an ambient atmosphere. Complete curing, without any unreacted oily residue on the surface of the silicone elastomer, was achieved in the absence of inert atmosphere protection. The impact of a formulation and photoinitiating system, including the use of visible-light initiators, on the kinetics and mechanical properties of the silicone networks was studied. Despite their opacity, nanocomposites incorporating fumed silica and graphene oxide (GO) retained fast cure rates (gelation times below 1 and 5 s for silica and GO composites, respectively) with tack-free surfaces. After thermal conversion, this afforded composites with conductivities above 0.1 S/m. Finally, combination with a conventional room-temperature vulcanization system enabled the formulation of effective dual-cure composites. The fast crosslinking thiol–norbornene silicones reported are attractive for a wide range of applications where ambient curing is required or where processing requires ultrafast reaction rates.

KeyWords AITranslate

silicone elastomer nanocomposite thiol−ene photochemistry norbornene
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00440

Chinese Library Classification Number:

Citation Information:

Photocured silicone elastomers have become increasingly popular in a variety of advanced materials applications including soft robotics, biomedical devices, microfabrication, functional coatings, and additive manufacturing. Oxygen inhibition, however, remains a major challenge for conventional photoradical curing, limiting applications and restricting processing. Here, we report a thiol–norbornene-based silicone system using a polydimethylsiloxane (PDMS) displaying terminal norbornene groups and a highly functionalized thiolated PDMS to achieve very fast curing speeds in an ambient atmosphere. Complete curing, without any unreacted oily residue on the surface of the silicone elastomer, was achieved in the absence of inert atmosphere protection. The impact of a formulation and photoinitiating system, including the use of visible-light initiators, on the kinetics and mechanical properties of the silicone networks was studied. Despite their opacity, nanocomposites incorporating fumed silica and graphene oxide (GO) retained fast cure rates (gelation times below 1 and 5 s for silica and GO composites, respectively) with tack-free surfaces. After thermal conversion, this afforded composites with conductivities above 0.1 S/m. Finally, combination with a conventional room-temperature vulcanization system enabled the formulation of effective dual-cure composites. The fast crosslinking thiol–norbornene silicones reported are attractive for a wide range of applications where ambient curing is required or where processing requires ultrafast reaction rates.

quote

GB/T 7714-2015 [1] Khai D. Q. Nguyen, Maria CrespoRibadeneyra, Olivier Picot, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00440.
MLA [1] Khai D. Q. Nguyen, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00440.
APA [1] Khai D. Q. Nguyen, Maria CrespoRibadeneyra, Olivier Picot, Burcu Colak, & Julien E. Gautrot. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00440