Description is made of the tension and compressiontests, deformation and fracture behavior of Nb - Mo - W alloy with different content of W. Mo.O and C.
KeyWords AITranslate
1Kin V Y,et al.Effect of Carbon on the tensite properties of Nb-Mo-W alloys at 1 773 K[J].Joural of Alloys and Compounds,2002,333:170.
1王慧利.电感耦合等离子体原子发射光谱法测定铌钨合金中钽[J].冶金分析,2014,34(6):49-52. 被引量:3
1李志伟,赵晓亮,李珍,王烨,王君玉.敞口酸熔-电感耦合等离子体发射光谱法测定稀有多金属矿选矿样品中的铌钽和伴生元素[J].岩矿测试,2017,36(6):594-600. 被引量:11
2张斯美,段宏然.电感耦合等离子体发射光谱法测定碳化铌中钽、钛含量[J].铁合金,2020,51(2):41-43.
3许宁辉,张众,张俊峰.电感耦合等离子体原子发射光谱法测定铌钨合金中钽硅铁铝钛铜[J].冶金分析,2021,41(1):80-86. 被引量:3
1К.,ВС,阎庆甲.钼钨合金在高温下的机械性能和断裂特性[J].钨钼材料,1990(4):32-36.
2徐掌印,张峰,姜银举.铈对1Cr17不锈钢夹杂物的影响[J].稀土,2010,31(2):48-50. 被引量:3
3吴明海,杨士浩.钼对中硅蠕铁高温机械性能的影响[J].现代铸铁,1991(2):38-40. 被引量:1
4朱自成,黄其慰.兵器用新身管钢高温机械性能测试[J].四川兵工学报,1990(4):231-237.
5王汝耀,鲁薇华,罗全顺.Cu、Mn、Fe、Mg等元素对活塞高温机械性能的影响[J].内燃机配件,1988(4):60-64.
6蒲正利.碳对Nb-Mo-W合金拉伸性能的影响[J].稀有金属快报,2003(3):24-24.
7黄金昌.合金元素对Nb-Mo-W合金性能的影响[J].稀有金属快报,2004(9):37-37.
8Yoshitaka Iwabuchi,慷为.13Cr-4Ni型铸钢的回火脆化现象[J].大型铸锻件,1988(2):81-88.
9赵沛廉,张金山.锰对ZA-27合金高温性能的影响[J].材料科学与工艺,1996,4(3):34-37. 被引量:17
10李有观.电阻率和加工性好的钼钨合金材料[J].世界有色金属,2005(5):68-68.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]
Citation Information:
Description is made of the tension and compressiontests, deformation and fracture behavior of Nb - Mo - W alloy with different content of W. Mo.O and C.
quote
| GB/T 7714-2015 | [1] YANG Yang. Impact of Mo and Carbon Content on the High-temperature Mechanical Property of Nb-Mo-W Alloy[J]. Rare Metals and Cemented Carbides, 2005(3): 59-61. |
| MLA | [1] YANG Yang. "Impact of Mo and Carbon Content on the High-temperature Mechanical Property of Nb-Mo-W Alloy." Rare Metals and Cemented Carbides, no. 3, 2005, pp. 59-61. |
| APA | [1] YANG Yang. (2005). Impact of Mo and Carbon Content on the High-temperature Mechanical Property of Nb-Mo-W Alloy. Rare Metals and Cemented Carbides(3), 59-61. |
| IEEE | [1] YANG Yang, "Impact of Mo and Carbon Content on the High-temperature Mechanical Property of Nb-Mo-W Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 59-61, 2005. keywords: {Nb - Mo - W alloy;mechanical property;fracture method;carbide precipitation} |