Effects of Y Doping on Magnetic Properties of Sm2Co17 Melt-Spun Ribbon AITranslate
Abstract AITranslate
A series of(Sm1-xYx)2Co17 melt-spun ribbons with different Y doping contents were prepared by the melt spinning method.XRD was employed to characterize the phase compositions of both the(Sm1-xYx)2Co17 alloy and its corresponding melt spun ribbons,while VSM was utilized to measure the magnetic properties of the ribbons.The results show that the(Sm1-xYx)2Co17 melt-spun ribbons mainly consist of(Sm,Y)2Co17 single phase.After melt spinning,the diffraction peak intensity of the(001)crystal plane is significantly enhanced,manifesting a distinct preferred orientation.The Sm2Co17 melt-spun ribbons fabricated at a spinning speed of 35 m/s exhibit the optimal magnetic properties,with a coercivity of 1022.5 Oe and a remanence of 29.3 emu/g.In addition,the easy magnetization direction of these ribbons is along the c-axis.With an increase in Y doping content,the magnetocrystalline anisotropy of the(Sm1-xYx)2Co17 melt-spun ribbons decreases,which consequently leads to a gradual reduction in both coercivity and remanence.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TG146.4[一般工业技术]
Citation Information:
A series of(Sm1-xYx)2Co17 melt-spun ribbons with different Y doping contents were prepared by the melt spinning method.XRD was employed to characterize the phase compositions of both the(Sm1-xYx)2Co17 alloy and its corresponding melt spun ribbons,while VSM was utilized to measure the magnetic properties of the ribbons.The results show that the(Sm1-xYx)2Co17 melt-spun ribbons mainly consist of(Sm,Y)2Co17 single phase.After melt spinning,the diffraction peak intensity of the(001)crystal plane is significantly enhanced,manifesting a distinct preferred orientation.The Sm2Co17 melt-spun ribbons fabricated at a spinning speed of 35 m/s exhibit the optimal magnetic properties,with a coercivity of 1022.5 Oe and a remanence of 29.3 emu/g.In addition,the easy magnetization direction of these ribbons is along the c-axis.With an increase in Y doping content,the magnetocrystalline anisotropy of the(Sm1-xYx)2Co17 melt-spun ribbons decreases,which consequently leads to a gradual reduction in both coercivity and remanence.
quote
| GB/T 7714-2015 | [1] FU Sen-yang, XU Cheng-fu, TANG Zhen, et al. Effects of Y Doping on Magnetic Properties of Sm2Co17 Melt-Spun Ribbon[J]. Rare Metals and Cemented Carbides, 2026(1): 67-71. |
| MLA | [1] FU Sen-yang, et al., "Effects of Y Doping on Magnetic Properties of Sm2Co17 Melt-Spun Ribbon." Rare Metals and Cemented Carbides, no. 1, 2026, pp. 67-71. |
| APA | [1] FU Sen-yang, XU Cheng-fu, TANG Zhen, YANG Yong-quan, MA Lei, LIU Rong-jin, DU Yu-song, & LI Lin. (2026). Effects of Y Doping on Magnetic Properties of Sm2Co17 Melt-Spun Ribbon. Rare Metals and Cemented Carbides(1), 67-71. |
| IEEE | [1] FU Sen-yang, XU Cheng-fu, TANG Zhen, YANG Yong-quan, MA Lei, LIU Rong-jin, DU Yu-song, and LI Lin, "Effects of Y Doping on Magnetic Properties of Sm2Co17 Melt-Spun Ribbon," Rare Metals and Cemented Carbides, no. 1, pp. 67-71, 2026. keywords: {SmCo;Y doping;melt spinning method;melt-spun ribbon;magnetic property;magnetocrystalline anisotropy} |