daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Photopolymerization and Photostructuring of Molecularly Imprinted Polymers AITranslate

Université de Technologie de Compiègne; France|Université de Strasbourg;Université de Technologie de Compiègne;Université de Technologie de Compiègne
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Over the past few decades, molecularly imprinted polymers (MIPs) have become extremely attractive materials for biomimetic molecular recognition due to their excellent affinity and specificity, combined with robustness, easy engineering, and competitive costs. MIPs are synthetic antibody mimics obtained by the synthesis of 3D polymer networks around template molecules, thus generating specific binding cavities. Numerous efforts have been made to improve the performances and the versatility of MIPs, with a special focus on ways to control their size, morphology, and physical form for a given application. Gaining control over these parameters has allowed MIPs to adopt a defined micro- and nanostructure, providing access to nanocomposites and micro/nanosystems, with fine-tuned properties, which become critical for modern applications ranging from chemical sensing to bioimaging and medical therapy. In this rich and complex context, light as a cheap and versatile source of energy has emerged as a powerful tool for structuring MIPs. This review presents the most recent advances on structuring MIPs at the nano/microscale, using light as a stimulus to trigger the polymerization process. Thus, after a general introduction on radical polymerization of MIPs, with a special emphasis on photopolymerization by UV and visible light, the reader will be presented with ways of structuring MIPs by processes that are inherently spatially confined, such as localized photopolymerization and lithographic techniques, supported by representative examples and complemented with a final outlook on future trends in this field.

KeyWords AITranslate

molecularly imprinted polymers photopolymerization photostructuring mask lithography maskless lithography stereolithography Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00661

Chinese Library Classification Number:

Citation Information:

Over the past few decades, molecularly imprinted polymers (MIPs) have become extremely attractive materials for biomimetic molecular recognition due to their excellent affinity and specificity, combined with robustness, easy engineering, and competitive costs. MIPs are synthetic antibody mimics obtained by the synthesis of 3D polymer networks around template molecules, thus generating specific binding cavities. Numerous efforts have been made to improve the performances and the versatility of MIPs, with a special focus on ways to control their size, morphology, and physical form for a given application. Gaining control over these parameters has allowed MIPs to adopt a defined micro- and nanostructure, providing access to nanocomposites and micro/nanosystems, with fine-tuned properties, which become critical for modern applications ranging from chemical sensing to bioimaging and medical therapy. In this rich and complex context, light as a cheap and versatile source of energy has emerged as a powerful tool for structuring MIPs. This review presents the most recent advances on structuring MIPs at the nano/microscale, using light as a stimulus to trigger the polymerization process. Thus, after a general introduction on radical polymerization of MIPs, with a special emphasis on photopolymerization by UV and visible light, the reader will be presented with ways of structuring MIPs by processes that are inherently spatially confined, such as localized photopolymerization and lithographic techniques, supported by representative examples and complemented with a final outlook on future trends in this field.

quote

GB/T 7714-2015 [1] Ernesto III Paruli, Olivier Soppera, Karsten Haupt, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00661.
MLA [1] Ernesto III Paruli, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00661.
APA [1] Ernesto III Paruli, Olivier Soppera, Karsten Haupt, & Carlo Gonzato. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00661
IEEE [1] Ernesto III Paruli, Olivier Soppera, Karsten Haupt, and Carlo Gonzato, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00661. keywords: {molecularly imprinted polymers;photopolymerization;photostructuring;mask lithography;maskless lithography;stereolithography;Show More}