In recent years, the Haber-Bosh process`s ammonia synthesis has shown a lot of energy consumption and significant CO2 emissions. In this sense, the photoelectrochemical production of NH3 via dinitrogen fixation has been showing a promising strategy. Thus, in this work, ammonia production under photoelectrocatalytic condition was carried out using the metal-organic iron terephthalate structure (MOF-235), obtained by a simple and low-cost process (solvothermal). The results indicated greater activity for the nitrogen reduction reaction (NRR) compared to the hydrogen reduction reaction (HRR), in addition to a high yield of NH3 0.716 µg h−1 cm−2 and Faradaic efficiency greater than 21.0% at - 0.2 V vs reversible hydrogen electrode in 0.1 mol L−1 Na2SO4 electrolyte. It is believed that the good results of MOF-235 during NRR are related to a high specific area of MOF, making available active sites of trinuclear-oxocentered iron in abundance. The material homogeneity in the electrode and the excellent light absorption were also decisive factors for the supply of high energy electrons necessary for ammonia production. Graphical Download : Download high-res image (130KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.apmt.2022.101540
Chinese Library Classification Number:
Citation Information:
In recent years, the Haber-Bosh process`s ammonia synthesis has shown a lot of energy consumption and significant CO2 emissions. In this sense, the photoelectrochemical production of NH3 via dinitrogen fixation has been showing a promising strategy. Thus, in this work, ammonia production under photoelectrocatalytic condition was carried out using the metal-organic iron terephthalate structure (MOF-235), obtained by a simple and low-cost process (solvothermal). The results indicated greater activity for the nitrogen reduction reaction (NRR) compared to the hydrogen reduction reaction (HRR), in addition to a high yield of NH3 0.716 µg h−1 cm−2 and Faradaic efficiency greater than 21.0% at - 0.2 V vs reversible hydrogen electrode in 0.1 mol L−1 Na2SO4 electrolyte. It is believed that the good results of MOF-235 during NRR are related to a high specific area of MOF, making available active sites of trinuclear-oxocentered iron in abundance. The material homogeneity in the electrode and the excellent light absorption were also decisive factors for the supply of high energy electrons necessary for ammonia production. Graphical Download : Download high-res image (130KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Luan Pereira Camargo, Paulo Rogério Catarini da Silva, Augusto BataginNeto, et al. Applied Materials Today, 2022(28). DOI:10.1016/j.apmt.2022.101540. |
| MLA | [1] Luan Pereira Camargo, et al., Applied Materials Today, no. 28, 2022, https://doi.org/10.1016/j.apmt.2022.101540. |
| APA | [1] Luan Pereira Camargo, Paulo Rogério Catarini da Silva, Augusto BataginNeto, Vanessa Klobukoski, Marcio Vidotti, & Luiz Henrique Dall`Antonia. (2022). Applied Materials Today(28). https://doi.org/10.1016/j.apmt.2022.101540 |
| IEEE | [1] Luan Pereira Camargo, Paulo Rogério Catarini da Silva, Augusto BataginNeto, Vanessa Klobukoski, Marcio Vidotti, and Luiz Henrique Dall`Antonia, Applied Materials Today, no. 28, 2022, doi: 10.1016/j.apmt.2022.101540. |