Study on Deep Cryogenic Treatment of WC-10Co Cemented Carbide as Cutting Tool Material AITranslate
Abstract AITranslate
The effect of deep cryogenic treatment on the wear resistance of WC-10Co lathe tool was studied with TC4 titanium alloy as the processed piece. The hardness and microstructure of the lathe tool were ana lyzed and tested by hardness tester,SEM and XRD. The research results show that the wear resistance of the lathe tool can be greatly improved by deep cryogenic treatment(DCT). With the increase of the turning length,the advantage of DTC lathe tool becomes more obvious. After deep cryogenic treatment, the hard ness of the lathe tool is slightly increased,the bending strength and toughness are significantly improved, and the microstructure is not obviously changed. The peak of WC in the XRD pattern of DTC lathe tool shifts to right, indicating that the compressive stress of WC decreases and the tensile stress of Co binder phase decreases,which is advantageous for increasing the strength of the alloy.
KeyWords AITranslate
1赵步青,胡明.我国刀具行业可持续发展战略之思考[J].金属加工:热加工,2014(19):22-25. 被引量:1
2赵宇龙.第三届切削刀具用户调查分析报告[J].金属加工:冷加工,2014(7):28-32. 被引量:1
3张劲松,袁子洲,刘秀芝,李士燕.金属材料深冷处理现状[J].甘肃工业大学学报,2003,29(1):32-35. 被引量:14
4陈红卫.深冷处理对硬质合金机械性能的影响[J].硬质合金,1995,12(1):33-36. 被引量:18
5刘寿荣,刘方.WC-Co硬质合金深冷处理强化机理[J].金属热处理学报,1997,18(4):57-60. 被引量:29
6陈振华,姜勇,樊恋,张忠健,徐涛,彭文.深冷处理对WC-Co硬质合金组织和性能的影响[J].材料热处理学报,2011,32(7):26-30. 被引量:17
7阎红娟,徐宏海,罗学科.YT15硬质合金刀片深冷处理工艺实验研究[J].制造技术与机床,2010(6):113-115. 被引量:11
1郭世柏,易正翼,段晓云,王南川,廖景冰.低温燃烧法制备(W,Mo)C/Al_(2)O_(3)/La_(2)O_(3)复合粉末及性能[J].材料工程,2021,49(3):133-140. 被引量:1
2易晓鸥,王方方,梁自强,陶星豪,辛浩翔.WC-Co硬质合金的深冷处理改性与显微机制[J].硬质合金,2021,38(3):219-228. 被引量:1
1鄢志刚,雷纯鹏,蔡海燕,吴爱华,唐建成.原料形貌特性和高温梯度碳化工艺对纳米WC粉末及其WC-Co合金均匀性的影响[J].硬质合金,2021,38(4):255-263. 被引量:1
2高峰.低碳经济中的燃煤电厂脱硫脱硝除尘工艺发展对策分析[J].电力设备管理,2022(8):209-211.
1马宇光.挂篮施工形式对斜拉桥应力影响及施工优化分析[J].兰州工业学院学报,2019,26(1):39-42.
2曾瑞霖,龙宁华,肖跃勇,罗胜,张卫兵,徐涛.硬质合金刀具材料主要物理力学性能对钛合金铣削加工的影响[J].硬质合金,2019,36(1):75-79. 被引量:2
3魏诗萌,孙杨,王福山,杨鑫华.搅拌摩擦焊搅拌头疲劳寿命的模拟研究[J].焊接技术,2019,48(4):5-9. 被引量:4
4周盼龙,肖代红,周鹏飞,余永新,袁珉慧.热压法制备超细晶WC-Al_xCrFeCoNi复合材料及其组织与性能[J].粉末冶金材料科学与工程,2019,24(2):100-105. 被引量:2
5闫自海,章立峰,路军富,邹金杰.城市地下立交隧道交叉口施工方法研究[J].现代隧道技术,2019,56(1):176-184. 被引量:15
6李琳.愿成为客户的全球工业解决方案合作伙伴[J].现代制造,2019,0(13):18-18.
7吴玖.森拉天时:全新品牌架构首度亮相[J].数控机床市场,2019,0(3):27-27.
8黄玉双.刻瓷艺术釉雕工艺和技法的创新[J].陶瓷科学与艺术,2019,53(2):51-54. 被引量:1
9李艳林,渠慎春,栾雨婷,高志红.苹果茎尖超低温脱毒体系的建立[J].分子植物育种,2019,17(9):2982-2995. 被引量:3
10仇建磊,贡金鑫.考虑屈曲影响的钢筋滞回本构模型[J].土木工程学报,2019,52(2):11-21. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG156.91[金属学及工艺—热处理]
Citation Information:
The effect of deep cryogenic treatment on the wear resistance of WC-10Co lathe tool was studied with TC4 titanium alloy as the processed piece. The hardness and microstructure of the lathe tool were ana lyzed and tested by hardness tester,SEM and XRD. The research results show that the wear resistance of the lathe tool can be greatly improved by deep cryogenic treatment(DCT). With the increase of the turning length,the advantage of DTC lathe tool becomes more obvious. After deep cryogenic treatment, the hard ness of the lathe tool is slightly increased,the bending strength and toughness are significantly improved, and the microstructure is not obviously changed. The peak of WC in the XRD pattern of DTC lathe tool shifts to right, indicating that the compressive stress of WC decreases and the tensile stress of Co binder phase decreases,which is advantageous for increasing the strength of the alloy.
quote
| GB/T 7714-2015 | [1] DONG Li-li, ZHANG Ning, WANG Lei, et al. Study on Deep Cryogenic Treatment of WC-10Co Cemented Carbide as Cutting Tool Material[J]. Rare Metals and Cemented Carbides, 2019(3): 86-90. |
| MLA | [1] DONG Li-li, et al., "Study on Deep Cryogenic Treatment of WC-10Co Cemented Carbide as Cutting Tool Material." Rare Metals and Cemented Carbides, no. 3, 2019, pp. 86-90. |
| APA | [1] DONG Li-li, ZHANG Ning, WANG Lei, MA Su-juan, & ZHANG He-jia. (2019). Study on Deep Cryogenic Treatment of WC-10Co Cemented Carbide as Cutting Tool Material. Rare Metals and Cemented Carbides(3), 86-90. |
| IEEE | [1] DONG Li-li, ZHANG Ning, WANG Lei, MA Su-juan, and ZHANG He-jia, "Study on Deep Cryogenic Treatment of WC-10Co Cemented Carbide as Cutting Tool Material," Rare Metals and Cemented Carbides, no. 3, pp. 86-90, 2019. keywords: {deep cryogenic treatment;cemented carbide;lathe tool;microscopic morphology;stress} |