Effect of Ultrasonic Vibration on the Melt-Spun Ribbon Boundary Region during Hot Deformation of Nd-Fe-B Magnets AITranslate

School of Mechanical and Electrical Engineering,Jiangxi University of Science and Technology;School of Mechanical and Electrical Engineering,Jiangxi University of Science and Technology;School of Mechanical and Electrical Engineering,Jiangxi University of Science and Technology;School of Mechanical and Electrical Engineering,Jiangxi University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To regulate the microstructure of the boundary region of the melt-spun ribbons in hot-deformed Nd-Fe-B magnets,ultrasonic vibration was applied during the hot deformation process of the Nd-Fe-B magnets.The microstructure of the melt-spun ribbon boundary region in the hot-pressed precursor was studied.The effects of conventional hot deformation and ultrasonic hot deformation on the distribution of the Nd-rich phase and the grain size in the melt-spun ribbon boundary region of Nd-Fe-B magnets were investigated,and the morphological evolution laws of the melt-spun ribbon boundary region were summarized.The results show that the microstructure of conventional hot-deformed Nd-Fe-B magnets retains the quasiperiodic distribution characteristics of the hot-pressed precursor's microstructure,with the continuously distributed strip-like Nd-rich phase at the periodic interface being wider.However,in the melt-spun ribbon boundary region in ultrasonic hot-deformed Nd-Fe-B magnets,the strip-like distribution of the Nd-rich phase is weakened.Instead,the Nd-rich phase gradually disperses and spreads toward the interior of the melt-spun ribbons,tending to distribute around the internal grains,which is conducive to improving the intergranular exchange coupling.In addition,compared with conventional hot-deformed Nd-Fe-B magnets,the grains in the coarse-grained region of the melt-spun ribbon boundary region in ultrasonic hot-deformed magnets are refined to a certain extent:the average grain size decreases from 2.17μm(conventional hot deformation)to 1.96μm(ultrasonic hot deformation),with a reduction of approximately 9.6%.

KeyWords AITranslate

hot deformation Nd-Fe-B magnet melt-spun ribbon boundary region ultrasonic vibration grain size Nd-rich phase
No data

Basic Information:

DOI:

Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]

Citation Information:

To regulate the microstructure of the boundary region of the melt-spun ribbons in hot-deformed Nd-Fe-B magnets,ultrasonic vibration was applied during the hot deformation process of the Nd-Fe-B magnets.The microstructure of the melt-spun ribbon boundary region in the hot-pressed precursor was studied.The effects of conventional hot deformation and ultrasonic hot deformation on the distribution of the Nd-rich phase and the grain size in the melt-spun ribbon boundary region of Nd-Fe-B magnets were investigated,and the morphological evolution laws of the melt-spun ribbon boundary region were summarized.The results show that the microstructure of conventional hot-deformed Nd-Fe-B magnets retains the quasiperiodic distribution characteristics of the hot-pressed precursor's microstructure,with the continuously distributed strip-like Nd-rich phase at the periodic interface being wider.However,in the melt-spun ribbon boundary region in ultrasonic hot-deformed Nd-Fe-B magnets,the strip-like distribution of the Nd-rich phase is weakened.Instead,the Nd-rich phase gradually disperses and spreads toward the interior of the melt-spun ribbons,tending to distribute around the internal grains,which is conducive to improving the intergranular exchange coupling.In addition,compared with conventional hot-deformed Nd-Fe-B magnets,the grains in the coarse-grained region of the melt-spun ribbon boundary region in ultrasonic hot-deformed magnets are refined to a certain extent:the average grain size decreases from 2.17μm(conventional hot deformation)to 1.96μm(ultrasonic hot deformation),with a reduction of approximately 9.6%.

quote

GB/T 7714-2015 [1] ZHU Ning-yuan, LI Zhi-qi, LOU Jia-le, et al. Effect of Ultrasonic Vibration on the Melt-Spun Ribbon Boundary Region during Hot Deformation of Nd-Fe-B Magnets[J]. Rare Metals and Cemented Carbides, 2025(6): 101-107.
MLA [1] ZHU Ning-yuan, et al., "Effect of Ultrasonic Vibration on the Melt-Spun Ribbon Boundary Region during Hot Deformation of Nd-Fe-B Magnets." Rare Metals and Cemented Carbides, no. 6, 2025, pp. 101-107.
APA [1] ZHU Ning-yuan, LI Zhi-qi, LOU Jia-le, & AO Fu-qiang. (2025). Effect of Ultrasonic Vibration on the Melt-Spun Ribbon Boundary Region during Hot Deformation of Nd-Fe-B Magnets. Rare Metals and Cemented Carbides(6), 101-107.
IEEE [1] ZHU Ning-yuan, LI Zhi-qi, LOU Jia-le, and AO Fu-qiang, "Effect of Ultrasonic Vibration on the Melt-Spun Ribbon Boundary Region during Hot Deformation of Nd-Fe-B Magnets," Rare Metals and Cemented Carbides, no. 6, pp. 101-107, 2025. keywords: {hot deformation;Nd-Fe-B magnet;melt-spun ribbon boundary region;ultrasonic vibration;grain size;Nd-rich phase}