daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fabrication of Cartilage-Inspired Hydrogel/Entangled Polymer–Elastomer Structures Possessing Poro-Elastic Properties AITranslate

University of Leeds; Imperial College London; University of Leeds; University of Leeds; Imperial College London; University of Leeds
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The ability to replicate the load-bearing properties of articular cartilage is attractive for many engineering applications, particularly bearings where low friction, low wear, and high durability are required. Hydrogels are widely used materials spanning many diverse applications owing to their lubricity and unique mechanical/chemical properties. The poor mechanical characteristics of conventional hydrogels, especially their compressive behavior, limit their application in load-bearing applications despite their favorable properties such as poro/viscoelasticity and lubricity. This paper demonstrates a cartilage-inspired approach to produce a structure that benefits from water-swelling resistant and ultrafast recovery behavior of elastomers as well as the stress-relaxation and energy dissipation properties of hydrogels. A method is presented in this work to fabricate interconnected macro-porous elastomers based on sintering poly(methyl methacrylate) beads. The porous elastomer imparted structural support and resilience to its composite with an infused-grafted hydrogel. At 30% strain and depending upon the strain rate, the composite exhibited a load-bearing behavior that was 14–19 times greater than that of pristine hydrogel and approximately 3 times greater than that of the porous elastomer. The equilibrium elastic modulus of the composite was 452 kPa at a strain range of 10%–30%, which was close to the values reported for the modulus of cartilage tested with similar experimental parameters defined in this study. The dissipated energy for the composite at strain rates of 1 and 10–3 s–1 was enhanced by 25-, 25-, 5-, and 15-fold as compared to that for the pristine hydrogel and the porous elastomer, respectively. The cyclic loading tests at two strain rates showed that the composite immediately recovers its load-bearing properties with the maximum load recovery staying above 95% of its initial values throughout the testing. The permeability of the structures was measured experimentally, and the results showed a decrease of permeability by 3 orders of magnitude following hydrogel grafting.

KeyWords AITranslate

poroelastic bioinspired hydrogel cartilage rehydration stress relaxation tough hydrogel composite polyacrylamide gel Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00256

Chinese Library Classification Number:

Citation Information:

The ability to replicate the load-bearing properties of articular cartilage is attractive for many engineering applications, particularly bearings where low friction, low wear, and high durability are required. Hydrogels are widely used materials spanning many diverse applications owing to their lubricity and unique mechanical/chemical properties. The poor mechanical characteristics of conventional hydrogels, especially their compressive behavior, limit their application in load-bearing applications despite their favorable properties such as poro/viscoelasticity and lubricity. This paper demonstrates a cartilage-inspired approach to produce a structure that benefits from water-swelling resistant and ultrafast recovery behavior of elastomers as well as the stress-relaxation and energy dissipation properties of hydrogels. A method is presented in this work to fabricate interconnected macro-porous elastomers based on sintering poly(methyl methacrylate) beads. The porous elastomer imparted structural support and resilience to its composite with an infused-grafted hydrogel. At 30% strain and depending upon the strain rate, the composite exhibited a load-bearing behavior that was 14–19 times greater than that of pristine hydrogel and approximately 3 times greater than that of the porous elastomer. The equilibrium elastic modulus of the composite was 452 kPa at a strain range of 10%–30%, which was close to the values reported for the modulus of cartilage tested with similar experimental parameters defined in this study. The dissipated energy for the composite at strain rates of 1 and 10–3 s–1 was enhanced by 25-, 25-, 5-, and 15-fold as compared to that for the pristine hydrogel and the porous elastomer, respectively. The cyclic loading tests at two strain rates showed that the composite immediately recovers its load-bearing properties with the maximum load recovery staying above 95% of its initial values throughout the testing. The permeability of the structures was measured experimentally, and the results showed a decrease of permeability by 3 orders of magnitude following hydrogel grafting.

quote

GB/T 7714-2015 [1] Siavash Soltanahmadi, Nicholas Raske, Gregory N. de Boer, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00256.
MLA [1] Siavash Soltanahmadi, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00256.
APA [1] Siavash Soltanahmadi, Nicholas Raske, Gregory N. de Boer, Anne Neville, Robert W. Hewson, & Michael G. Bryant. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00256
IEEE [1] Siavash Soltanahmadi, Nicholas Raske, Gregory N. de Boer, Anne Neville, Robert W. Hewson, and Michael G. Bryant, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00256. keywords: {poroelastic;bioinspired hydrogel;cartilage rehydration;stress relaxation;tough hydrogel composite;polyacrylamide gel;Show More}