Correction to “Degradable Thermoset Fibers from Carbohydrate-Derived Diols via Thiol–Ene Photopolymerization” AITranslate

AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00770

Chinese Library Classification Number:

Citation Information:

quote

GB/T 7714-2015 [1] SungSoo Kim, C. Maggie Lau, Leon M. Lillie, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00770.
MLA [1] SungSoo Kim, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00770.
APA [1] SungSoo Kim, C. Maggie Lau, Leon M. Lillie, William B. Tolman, Theresa M. Reineke, & Christopher J. Ellison. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00770