Proportional Optimization Model of Multiscale Spherical BN for Enhancing Thermal Conductivity Proportional Optimization Model of Multiscale Spherical BN for Enhancing Thermal Conductivity AITranslate
Abstract AITranslate
The power electronics tend to become miniaturized and multifunctionalized, such as thermal rotators, circuit breakers, and microchips, which have necessitated creating instruments for investigating thermal mechanisms and enhancing thermal conductivity. In this paper, we construct the heat flow network of spherical boron nitride (BN) and used multiscale spherical BN to improve the thermal conductivity of the composite synergistically. The multiscale spherical filler ratio optimization model based on the Dinger–Funk particle stacking theory is established, which obtained the optimal volume ratio of 0.224:0.374:0.402 with D50 of 20, 70, and 160 μm. Meanwhile, the effects of multiscale filler ratio, morphology, filler content, and temperature are investigated. The thermal conductivity of composites can reach up to 1.84 W/(m·K) at 20 vol %. Significantly, the thermal conductivity of composites is 4.82 W/(m·K) at 30 vol %, which is achieved by optimizing the multiscale filler and particle size distribution.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00878
Chinese Library Classification Number:
Citation Information:
The power electronics tend to become miniaturized and multifunctionalized, such as thermal rotators, circuit breakers, and microchips, which have necessitated creating instruments for investigating thermal mechanisms and enhancing thermal conductivity. In this paper, we construct the heat flow network of spherical boron nitride (BN) and used multiscale spherical BN to improve the thermal conductivity of the composite synergistically. The multiscale spherical filler ratio optimization model based on the Dinger–Funk particle stacking theory is established, which obtained the optimal volume ratio of 0.224:0.374:0.402 with D50 of 20, 70, and 160 μm. Meanwhile, the effects of multiscale filler ratio, morphology, filler content, and temperature are investigated. The thermal conductivity of composites can reach up to 1.84 W/(m·K) at 20 vol %. Significantly, the thermal conductivity of composites is 4.82 W/(m·K) at 30 vol %, which is achieved by optimizing the multiscale filler and particle size distribution.
quote
| GB/T 7714-2015 | [1] Senyuan Yang, Zhengyong Huang, Qinghua Hu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00878. |
| MLA | [1] Senyuan Yang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00878. |
| APA | [1] Senyuan Yang, Zhengyong Huang, Qinghua Hu, Yingfan Zhang, Feipeng Wang, Haohuan Wang, & Yingying Shu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00878 |
| IEEE | [1] Senyuan Yang, Zhengyong Huang, Qinghua Hu, Yingfan Zhang, Feipeng Wang, Haohuan Wang, and Yingying Shu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00878. keywords: {epoxy resin spherical BN multiscale proportional optimization thermal conductivity} |