daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Polymer-Based Devices and Remediation Strategies for Emerging Contaminants in Water AITranslate

Hacettepe University; The University of Alabama; The University of Alabama; The University of Alabama; Amirkabir University of Technology; The University of Alabama; The University of Alabama; The University of Alabama; The University of Alabama
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The capturing of water contaminants and the remediation of water bodies is an important concern to human health due to severe side effects of contaminants on the body such as cancer. Pharmaceuticals, heavy metals, dyes, and chemical warfare agents (CWAs) are a few of the toxic pollutants that cause serious damage to the environment, humans, and animals. Meanwhile, scientists in the fields of polymer nanotechnology and nanoscience have been investigating tremendous solutions for eliminating water pollution to ensure environmental safety. Among all methods of water purification, adsorption is an important and versatile technique for remediation and has been used to remove toxic elements from water-based materials for many years. Using polymer-based materials as an adsorbent is very common to purify polluted waters. The main factors to evaluate adsorbent performance are adsorption capacity (maximum contaminant uptake by adsorbent), adsorption rate (how fast the adsorbent adsorbs contaminants), contaminant selectivity (adsorption of a specific contaminant among other ones), and adsorbent reusability (ability of adsorbent to remove contaminants in consecutive order), which are compared in this work. These factors are affected by pH, temperature, contact time, and also type, dosage, and morphology of the adsorbent. Natural and synthetic polymers in different types of films, membranes, nanocomposites, porous materials, and hydrogels with functional groups such as hydroxyl, amine, carboxyl, and amide are used as a selective material to adsorb water contaminants. Serious needs to remediate the water base from several contaminants direct the researchers to utilize polymer-based adsorbents with the ability to adsorb multiple contaminants simultaneously in the shortest possible time. This work reviews different water contaminants and their removal mechanisms and detection using nanodevices and polymer-based adsorbents.

KeyWords AITranslate

pharmaceuticals heavy metals dyes chemical warfare agents water remediation devices
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01171

Chinese Library Classification Number:

Citation Information:

The capturing of water contaminants and the remediation of water bodies is an important concern to human health due to severe side effects of contaminants on the body such as cancer. Pharmaceuticals, heavy metals, dyes, and chemical warfare agents (CWAs) are a few of the toxic pollutants that cause serious damage to the environment, humans, and animals. Meanwhile, scientists in the fields of polymer nanotechnology and nanoscience have been investigating tremendous solutions for eliminating water pollution to ensure environmental safety. Among all methods of water purification, adsorption is an important and versatile technique for remediation and has been used to remove toxic elements from water-based materials for many years. Using polymer-based materials as an adsorbent is very common to purify polluted waters. The main factors to evaluate adsorbent performance are adsorption capacity (maximum contaminant uptake by adsorbent), adsorption rate (how fast the adsorbent adsorbs contaminants), contaminant selectivity (adsorption of a specific contaminant among other ones), and adsorbent reusability (ability of adsorbent to remove contaminants in consecutive order), which are compared in this work. These factors are affected by pH, temperature, contact time, and also type, dosage, and morphology of the adsorbent. Natural and synthetic polymers in different types of films, membranes, nanocomposites, porous materials, and hydrogels with functional groups such as hydroxyl, amine, carboxyl, and amide are used as a selective material to adsorb water contaminants. Serious needs to remediate the water base from several contaminants direct the researchers to utilize polymer-based adsorbents with the ability to adsorb multiple contaminants simultaneously in the shortest possible time. This work reviews different water contaminants and their removal mechanisms and detection using nanodevices and polymer-based adsorbents.

quote

GB/T 7714-2015 [1] Saeideh Alipoori, Hadi Rouhi, Emily Linn, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01171.
MLA [1] Saeideh Alipoori, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01171.
APA [1] Saeideh Alipoori, Hadi Rouhi, Emily Linn, Hannah Stumpfl, Hadi Mokarizadeh, Milad Rabbani Esfahani, Amanda Koh, Steven T. Weinman, & Evan K. Wujcik. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01171
IEEE [1] Saeideh Alipoori, Hadi Rouhi, Emily Linn, Hannah Stumpfl, Hadi Mokarizadeh, Milad Rabbani Esfahani, Amanda Koh, Steven T. Weinman, and Evan K. Wujcik, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01171. keywords: {pharmaceuticals;heavy metals;dyes;chemical warfare agents;water remediation;devices}