The Latest Development of Preparation Methods of W-Cu Composite Materials AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The latest development of the preparation methods for W-Cu composite materials is reviewed, mainly including molten infiltration, chemical co-precipitation, mechanical alloying, hot-press sintering, co- reduction sintering, and sol-gel method. Meanwhile, the future development of W-Cu composite materials is pointed out.

KeyWords AITranslate

W-Cu composite material^preparation method density the latest development

1陈文革 谷臣清.封装用钨铜材料的制备技术.电器技术,1997,20(2):12-17.

2Upadhyaya A,German R M. Densification and dilation of sintered W-Cu alloys[J]. International Journal of Powder Metallurgy, 1998,84 (2) :43-55.

3王志法,刘正春,姜国圣.W-Cu电子封装材料的气密性[J].中国有色金属学报,1999,9(2):323-326. 被引量:59

4Johnson J L, German R M. Advance in powder metallurgy and particulate materials[J]. International Journal of Powder Metallurgy, 1993,29(4):201-209.

5吕大铭.钨基高密度合金强化研究的动向和进展[J].稀有金属材料与工程,1998,27:16-16.

6Kim J C,Ryu S S,Lee H,et al. Metal injection molding of nanostructured W-Cu composite powder[J]. The International Journal of Powder Metallurgy, 1999,35 (4) : 47-55.

7Kim J C, Moon I H. Sintering of nanostructured W-Cu alloys prepared by mechanical alloying[J]. Nanostructu- red Mater,1998,10(2):283-290.

8Hong S H,Kim B K. Fabrication of W-20wt% Cu com- posite nanopowder and sintered alloy with high thermal conductivity [ J ]. Materials Letters, 2003, 57:2 761- 2 767.

9姚惠龙,林涛,罗骥,刘祥庆,郭志猛.化学共沉淀法制备钨铜合金[J].稀有金属材料与工程,2009,38(2):348-352. 被引量:21

10Bhalla A K, Williams J D. A comparative assessment of explosive and other methods of compaction in the production of tungsten copper composite[J]. Powder Metallurgy, 1976, (1) : 31-37.

1王晖,张小明,王峰,蔡小梅,郑欣,李来平.W-Cu材料的应用进展和制备技术[J].硬质合金,2014,31(5):322-326. 被引量:8

2徐竹.钨铜复合材料制备技术的发展与应用[J].新技术新工艺,2016(6):76-78. 被引量:6

3沈晓,程继贵,李剑峰,陈闻超,卫陈龙,罗来马,吴玉程.轧膜成形制备W-Cu层状功能梯度材料及其性能研究[J].粉末冶金工业,2016,26(6):8-14. 被引量:6

4张保红,林冰涛,唐亮亮.难熔金属浸渗复合材料力学性能和抗烧蚀性能研究[J].中国钼业,2017,41(5):49-52. 被引量:6

5宫鑫,任帅,李黎.钨铜合金电触头材料的最新研究进展[J].广东电力,2019,32(5):87-98. 被引量:8

6崔同磊,张桂香,崔运涛,姜林志,滕潇,杜嘉静.响应曲面法优化铜钨合金材料的磁力光整加工参数[J].电镀与涂饰,2020,39(17):1209-1214. 被引量:6

7吕冬冬,鲍瑞,郭圣达,张建波,刘柏雄,陈俏.钨铜合金制备与应用研究[J].中国钨业,2021,36(5):65-77. 被引量:2

1徐竹.钨铜复合材料制备技术的发展与应用[J].新技术新工艺,2016(6):76-78. 被引量:6

2杨东麟,李达人,蔡一湘.粉末温轧工艺对W-20Cu合金密度和显微组织的影响[J].粉末冶金材料科学与工程,2016,21(3):470-474. 被引量:1

3沈晓,程继贵,李剑峰,陈闻超,卫陈龙,罗来马,吴玉程.轧膜成形制备W-Cu层状功能梯度材料及其性能研究[J].粉末冶金工业,2016,26(6):8-14. 被引量:6

4张景杰,刘兴亚.光伏电力开关用W-25Cu复合材料的微观组织和抗电弧侵蚀性研究[J].粉末冶金工业,2017,27(4):40-43.

5陶庆良,魏瑶瑶,李邦怿,谢海林,吴坷,朱玉斌.凝胶注模法制备复杂形状钨铜复合材料[J].稀有金属与硬质合金,2017,45(4):28-33. 被引量:3

6张保红,林冰涛,唐亮亮.难熔金属浸渗复合材料力学性能和抗烧蚀性能研究[J].中国钼业,2017,41(5):49-52. 被引量:6

7王巍,王军,张晓旭.水热还原法制备车电极用W-Cu复合粉末的特性表征[J].粉末冶金工业,2018,28(2):8-11. 被引量:3

8宫鑫,任帅,李黎.钨铜合金电触头材料的最新研究进展[J].广东电力,2019,32(5):87-98. 被引量:8

9左碧强,丁文红,贺文健,毋刚.钛粉轧制成形工艺研究[J].粉末冶金工业,2019,29(3):13-16. 被引量:6

10唐亮亮,刘国辉,张保红,林冰涛.钼含量对钨钼渗铜材料烧结工艺和力学性能的影响[J].中国钼业,2020,44(1):49-53. 被引量:2

1吴泓,王志法,姜国圣,崔大田,郑秋波.钨粉化学镀铜对W/15Cu电子封装材料性能的影响[J].稀有金属材料与工程,2007,36(3):550-553. 被引量:10

2宋贝贝,刘玉德,付传起,吴刚,张浩,王硕.MoS2对Fe-20wt%Cu基摩擦材料摩擦磨损性能的影响[J].热加工工艺,2016,45(24):52-56. 被引量:1

3梁冬冬,李德俭,于同庆.硬质合金复合刀具的制备及性能研究[J].铸造技术,2016,37(12):2654-2656. 被引量:1

4刘舒,谢敬佩,马窦琴,王凤梅,王爱琴,李继文,王文焱,孙浩亮,王维,程光耀.纳米钨铜复合粉末的制备及其烧结行为研究[J].稀有金属与硬质合金,2014,42(5):34-38. 被引量:11

5张会杰,李继文,魏世忠,潘昆明,王展,万成.超细晶W-Cu复合材料的热挤压与热处理[J].粉末冶金材料科学与工程,2016,21(1):25-34. 被引量:4

6范景莲,彭石高,刘涛,成会朝.钨铜复合材料的应用与研究现状[J].稀有金属与硬质合金,2006,34(3):30-35. 被引量:45

7徐凯.钨铜复合材料的现状与发展[J].中国钨业,2010,25(3):30-34. 被引量:19

8李云平,曲选辉,郑洲顺,雷长明.氧化-球磨-还原法制备超细弥散分布钨铜复合粉末[J].粉末冶金材料科学与工程,2003,8(3):242-246. 被引量:2

9王玲玲,方林霞,刘雪,吴志伟,崔庆荣.钨铜合金制备工艺分析[J].广州化工,2012,40(4):10-11. 被引量:3

10吴化波,王志法,刘金文,崔大田,姜国圣,周俊.钨铜材料电镀镍层常见缺陷分析及解决方法[J].表面技术,2008,37(3):80-83. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]

Citation Information:

The latest development of the preparation methods for W-Cu composite materials is reviewed, mainly including molten infiltration, chemical co-precipitation, mechanical alloying, hot-press sintering, co- reduction sintering, and sol-gel method. Meanwhile, the future development of W-Cu composite materials is pointed out.

quote

GB/T 7714-2015 [1] ZHAO Jing-jing, LI Ji-wen, ZHANG Pan-long, et al. The Latest Development of Preparation Methods of W-Cu Composite Materials[J]. Rare Metals and Cemented Carbides, 2013(4): 52-54.
MLA [1] ZHAO Jing-jing, et al., "The Latest Development of Preparation Methods of W-Cu Composite Materials." Rare Metals and Cemented Carbides, no. 4, 2013, pp. 52-54.
APA [1] ZHAO Jing-jing, LI Ji-wen, ZHANG Pan-long, & WEI Shi-zhong. (2013). The Latest Development of Preparation Methods of W-Cu Composite Materials. Rare Metals and Cemented Carbides(4), 52-54.
IEEE [1] ZHAO Jing-jing, LI Ji-wen, ZHANG Pan-long, and WEI Shi-zhong, "The Latest Development of Preparation Methods of W-Cu Composite Materials," Rare Metals and Cemented Carbides, no. 4, pp. 52-54, 2013. keywords: {W-Cu composite material^preparation method;density;the latest development}