Proximity-Induced Superconductivity in Atomically Precise Nanographene on Ag/Nb(110) AITranslate
Abstract AITranslate
Obtaining a robust superconducting state in atomically precise nanographene (NG) structures by proximity to a superconductor could foster the discovery of topological superconductivity in graphene. On-surface synthesis of such NGs has been achieved on noble metals and metal oxides; however, it is still absent on superconductors. Here, we present a synthetic method to induce superconductivity of polymeric chains and NGs adsorbed on the superconducting Nb(110) substrate covered by thin Ag films. Using atomic force microscopy at low temperature, we characterize the chemical structure of each subproduct formed on the superconducting Ag layer. Scanning tunneling spectroscopy further allows us to elucidate the electronic properties of these nanostructures, which consistently show a superconducting gap.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.2c00955
Chinese Library Classification Number:
Citation Information:
Obtaining a robust superconducting state in atomically precise nanographene (NG) structures by proximity to a superconductor could foster the discovery of topological superconductivity in graphene. On-surface synthesis of such NGs has been achieved on noble metals and metal oxides; however, it is still absent on superconductors. Here, we present a synthetic method to induce superconductivity of polymeric chains and NGs adsorbed on the superconducting Nb(110) substrate covered by thin Ag films. Using atomic force microscopy at low temperature, we characterize the chemical structure of each subproduct formed on the superconducting Ag layer. Scanning tunneling spectroscopy further allows us to elucidate the electronic properties of these nanostructures, which consistently show a superconducting gap.
quote
| GB/T 7714-2015 | [1] JungChing Liu, Rémy Pawlak, Xing Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00955. |
| MLA | [1] JungChing Liu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00955. |
| APA | [1] JungChing Liu, Rémy Pawlak, Xing Wang, Hongyan Chen, Philipp D’Astolfo, Carl Drechsel, Ping Zhou, Robert Häner, Silvio Decurtins, Ulrich Aschauer, ShiXia Liu, Wulf Wulfhekel, & Ernst Meyer. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00955 |
| IEEE | [1] JungChing Liu, Rémy Pawlak, Xing Wang, Hongyan Chen, Philipp D’Astolfo, Carl Drechsel, Ping Zhou, Robert Häner, Silvio Decurtins, Ulrich Aschauer, ShiXia Liu, Wulf Wulfhekel, and Ernst Meyer, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00955. |