daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Impact of Processing Methods on the Mechanical Properties and Texture of Ta Slab AITranslate

School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect of the processing methods on the mechanical properties of tantalum sheets was investigated in this paper.The microstructure of tantalum was observed under metallograph (OM). Also the texture of tantalum was tested by X - ray diffractometry.The results show that primary tandem rolling reduced the anisotropic properties of tantalum sheets and led to finer grain for tantalum sheets more effectively, provided tantalum with strong{ 111 } 〈 uvw〉 texture, the process is selected for the processing of tantalum plate for Ta electrolytic capacitor crust.

KeyWords AITranslate

processing method tantalum slab mechanic property texture

1张新明,张少睿,周卓平,舒永春.钽丝的拉拔及退火织构[J].中国有色金属学报,1999,9(4):774-778. 被引量:11

2刘枚.格沃利亚公司钽产量创新记录[J].稀有金属快报,1998,(7):22-22.

3Clark J B,et al.Influence of initial ingot breakdown on the microstructural and textural development of high-purity tantalum[J]. Metallurgical Transaction A,1991,22A:2 959.

4Clark J B,et al.Influence of transverse rolling on the microstructural and texture development in pure tantalum[J].metallurgical transaction A,1992,23A:2 183.

1张炎,王再友,查光成.热处理对钽板组织和力学性能的影响[J].热加工工艺,2011,40(24):218-221. 被引量:2

2潘文高,陈炜晔,吴澜尔.钽材轧制和再结晶织构演变研究进展[J].材料导报,2016,30(21):150-156.

3韩晨,孙付涛.钽铌板带生产与应用分析[J].有色金属加工,2017,46(5):7-12. 被引量:2

4徐潇敏,刘宁,刘爱军,严骏.钽及钽合金的制备方法和力学性能研究[J].热处理,2019,34(1):6-11. 被引量:6

5周永强,冯杉杉,朱政强.钽与不锈钢异种材料焊接的研究进展[J].电焊机,2023,53(1):63-70.

6殷子清,韩修柱,李景利,罗文博,孔钦可,王谦,胡励,薛志勇.中温轧制制备镁/铝/钽多层复合材料的界面扩散与力学性能研究[J].精密成形工程,2023,15(3):55-63.

1王跃,董凯,焦亮亮,王振华.深冷轧工艺在高性能金属材料制备中的应用[J].造纸装备及材料,2021,50(7):44-46. 被引量:1

2季良,杨武雄,肖荣诗.金属钽箔十字交叉激光微点焊工艺研究[J].应用激光,2013,33(6):601-605. 被引量:2

3韩晨,孙付涛.高抗力金属板带材多辊冷轧机特点分析[J].有色金属材料与工程,2018,39(5):33-38. 被引量:3

4马晶,李蛟,龚小涛,耿佩,周超.电子束熔炼工艺对Ta铸锭表面质量的影响[J].真空,2020,57(6):45-47.

5邓朝阳,闫星辰,董东东,王岳亮,马文有,刘敏.医用纯钽激光选区熔化制备工艺及力学性能研究[J].热加工工艺,2021,50(20):76-81. 被引量:1

6李涌泉,梁国栋,秦春,蒋亮,董福元,李宁.钽合金表面硅化物渗层的高温抗氧化性能[J].稀有金属,2021,45(9):1148-1152. 被引量:1

7张倩,李秀青,魏世忠,王琪,张程,徐流杰,周玉成.冷变形及退火对Ta-2.5W合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2022,50(2):50-56.

8刘新利,宋晓毓,王德志.铌/钢和钽/钛/钢层状复合材料中铌层和钽层的氢化剥离回收[J].稀有金属与硬质合金,2022,50(6):59-67.

9梁静,李延超,林小辉,张新,薛建嵘.样品尺寸对真空热处理后粉末冶金Ta-10W合金性能的影响[J].中国钨业,2022,37(4):54-60.

1袁韧,张新明,周卓平.退火温度对钽丝再结晶织构的影响[J].稀有金属与硬质合金,2002,30(3):17-21. 被引量:2

2袁韧,张新明,周卓平.钽丝的织构和再结晶行为研究[J].材料导报,2002,16(6):68-70. 被引量:2

3曹寒松.提高细径钽丝抗脆性的研究[J].稀有金属与硬质合金,1998,26(3):16-21. 被引量:1

4朱一民,赵晓红,严心羽.快速漏流分选仪[J].测控自动化,2005(1):51-52.

5刘建清,李荐,戴艳阳,钟海云.固体钽电解电容器研究发展趋势[J].稀有金属与硬质合金,2002,30(2):41-44. 被引量:6

6张声飞.高频固体钽电解电容器电性能与钽粉[J].电子元件与材料,1999,18(1):39-41. 被引量:3

7程越伟,郑爱国,潘伦桃,李慧,任萍.电容器用钽粉的高比容化[J].宁夏工程技术,2006,5(1):99-101. 被引量:12

Basic Information:

DOI:

Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]

Citation Information:

The effect of the processing methods on the mechanical properties of tantalum sheets was investigated in this paper.The microstructure of tantalum was observed under metallograph (OM). Also the texture of tantalum was tested by X - ray diffractometry.The results show that primary tandem rolling reduced the anisotropic properties of tantalum sheets and led to finer grain for tantalum sheets more effectively, provided tantalum with strong{ 111 } 〈 uvw〉 texture, the process is selected for the processing of tantalum plate for Ta electrolytic capacitor crust.

quote

GB/T 7714-2015 [1] GUO Lei, WANG Zhi-fa. Impact of Processing Methods on the Mechanical Properties and Texture of Ta Slab[J]. Rare Metals and Cemented Carbides, 2005(3): 18-22.
MLA [1] GUO Lei, and WANG Zhi-fa. "Impact of Processing Methods on the Mechanical Properties and Texture of Ta Slab." Rare Metals and Cemented Carbides, no. 3, 2005, pp. 18-22.
APA [1] GUO Lei, & WANG Zhi-fa. (2005). Impact of Processing Methods on the Mechanical Properties and Texture of Ta Slab. Rare Metals and Cemented Carbides(3), 18-22.
IEEE [1] GUO Lei and WANG Zhi-fa, "Impact of Processing Methods on the Mechanical Properties and Texture of Ta Slab," Rare Metals and Cemented Carbides, no. 3, pp. 18-22, 2005. keywords: {processing method;tantalum slab;mechanic property;texture}