CALF-20 is a zinc-triazole-oxalate-based metal–organic framework (MOF) that exhibits selective CO2 physisorption, which makes it attractive for potential applications in CO2 capture. However, to implement such applications, the CALF-20 structure must endure extended exposure to environmental conditions that may lead to changes in structure, chemistry, and, hence, performance. Here we find that the originally reported CALF-20 phase (now denoted α-CALF-20) undergoes a structure transformation following exposure to humid environments to generate a new polymorph, β-CALF-20, identified here through combined synchrotron powder X-ray diffraction and pair distribution function (PDF) analysis. This α-to-β transformation is fully reversible with α-CALF-20 being regenerated by treating β-CALF-20 under dry air or vacuum. The rapid reversion of β- to α-CALF-20 under conditions relevant to measuring the gas adsorption isotherm required the CO2 adsorption properties for β-CALF-20 to be evaluated computationally. Experimental evaluation of the adsorption behavior of β-CALF-20 is not practical. These analyses suggest that β-CALF-20 has a higher CO2 heat of adsorption than α-CALF-20, which may be advantageous to CO2 sorption selectivity at low partial pressures.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c00930
Chinese Library Classification Number:
Citation Information:
CALF-20 is a zinc-triazole-oxalate-based metal–organic framework (MOF) that exhibits selective CO2 physisorption, which makes it attractive for potential applications in CO2 capture. However, to implement such applications, the CALF-20 structure must endure extended exposure to environmental conditions that may lead to changes in structure, chemistry, and, hence, performance. Here we find that the originally reported CALF-20 phase (now denoted α-CALF-20) undergoes a structure transformation following exposure to humid environments to generate a new polymorph, β-CALF-20, identified here through combined synchrotron powder X-ray diffraction and pair distribution function (PDF) analysis. This α-to-β transformation is fully reversible with α-CALF-20 being regenerated by treating β-CALF-20 under dry air or vacuum. The rapid reversion of β- to α-CALF-20 under conditions relevant to measuring the gas adsorption isotherm required the CO2 adsorption properties for β-CALF-20 to be evaluated computationally. Experimental evaluation of the adsorption behavior of β-CALF-20 is not practical. These analyses suggest that β-CALF-20 has a higher CO2 heat of adsorption than α-CALF-20, which may be advantageous to CO2 sorption selectivity at low partial pressures.
quote
| GB/T 7714-2015 | [1] Zhihengyu Chen, ChingHwa Ho, Xiaoliang Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00930. |
| MLA | [1] Zhihengyu Chen, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00930. |
| APA | [1] Zhihengyu Chen, ChingHwa Ho, Xiaoliang Wang, Simon M. Vornholt, Thomas M. Rayder, Timur Islamoglu, Omar K. Farha, Francesco Paesani, & Karena W. Chapman. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00930 |
| IEEE | [1] Zhihengyu Chen, ChingHwa Ho, Xiaoliang Wang, Simon M. Vornholt, Thomas M. Rayder, Timur Islamoglu, Omar K. Farha, Francesco Paesani, and Karena W. Chapman, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00930. |