Synthesis of Pyrene-Based Covalent Organic Frameworks for Photocatalytic Tetracycline Degradation AITranslate

Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology; Central South University of Forestry and Technology; Hunan University; Hunan University; Hunan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Pyrene-based covalent organic frameworks (sp2c-COF and Py-NH2–COF) were successfully prepared via a solvothermal route. Upon the irradiation of visible light, COFs were used to degrade tetracycline hydrochloride (TC) in aqueous solution. The results showed that sp2c-COF exhibited much better photocatalytic activity than Py-NH2–COF. 73.5 and 3.1% TC could be degraded within 90.0 min with the initial concentration of 20 mg/L via sp2c-COF and py-NH2–COF under visible-light irradiation, respectively. The influence of bond connection types on the visible-light catalytic ability of COFs was explored. Electrochemical impedance spectroscopy (EIS) results proved that sp2c-COF had a higher photogenerated electron–hole separation efficiency. X-ray photoelectron spectroscopy (XPS) and Mott–Schottky plots revealed that the band gaps of sp2c-COF and Py-NH2–COF were 1.98 and 2.28 eV, respectively, resulting in sp2c-COF having a higher electron carrier transport efficiency. Importantly, sp2c-COF exhibits good reusability, affording 70.3% degradation efficiency even after 5 successive recycles. Active species trapping experiments and electron paramagnetic resonance (EPR) and electrochemical analyses were performed to consult the proposed degradation mechanism. This work indicates that the COF with C═C bonds could improve electron hole separation and electron carrier transport more effectively than the COF with C═N bonds in the photocatalytic process, which led to a more effective way of transmission of π conjugation across the two-dimensional (2D) lattice and thus enhanced the electron delocalization. So it was more beneficial for the degradation of tetracycline.

KeyWords AITranslate

photocatalysis COF tetracycline degradation visible light nonmetallic semiconductor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01765

Chinese Library Classification Number:

Citation Information:

Pyrene-based covalent organic frameworks (sp2c-COF and Py-NH2–COF) were successfully prepared via a solvothermal route. Upon the irradiation of visible light, COFs were used to degrade tetracycline hydrochloride (TC) in aqueous solution. The results showed that sp2c-COF exhibited much better photocatalytic activity than Py-NH2–COF. 73.5 and 3.1% TC could be degraded within 90.0 min with the initial concentration of 20 mg/L via sp2c-COF and py-NH2–COF under visible-light irradiation, respectively. The influence of bond connection types on the visible-light catalytic ability of COFs was explored. Electrochemical impedance spectroscopy (EIS) results proved that sp2c-COF had a higher photogenerated electron–hole separation efficiency. X-ray photoelectron spectroscopy (XPS) and Mott–Schottky plots revealed that the band gaps of sp2c-COF and Py-NH2–COF were 1.98 and 2.28 eV, respectively, resulting in sp2c-COF having a higher electron carrier transport efficiency. Importantly, sp2c-COF exhibits good reusability, affording 70.3% degradation efficiency even after 5 successive recycles. Active species trapping experiments and electron paramagnetic resonance (EPR) and electrochemical analyses were performed to consult the proposed degradation mechanism. This work indicates that the COF with C═C bonds could improve electron hole separation and electron carrier transport more effectively than the COF with C═N bonds in the photocatalytic process, which led to a more effective way of transmission of π conjugation across the two-dimensional (2D) lattice and thus enhanced the electron delocalization. So it was more beneficial for the degradation of tetracycline.

quote

GB/T 7714-2015 [1] Zhiyi Hu, Yong Luo, Lizhi Wang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01765.
MLA [1] Zhiyi Hu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01765.
APA [1] Zhiyi Hu, Yong Luo, Lizhi Wang, Yuanlan Wang, Qiong Wang, Guofang Jiang, Qianfan Zhang, & Fuzhi Cui. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01765
IEEE [1] Zhiyi Hu, Yong Luo, Lizhi Wang, Yuanlan Wang, Qiong Wang, Guofang Jiang, Qianfan Zhang, and Fuzhi Cui, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01765. keywords: {photocatalysis;COF;tetracycline degradation;visible light;nonmetallic semiconductor}