Self-Powered Electronic Skin for Remote Human–Machine Synchronization Self-Powered Electronic Skin for Remote Human–Machine Synchronization AITranslate

Qingdao University; China University of Petroleum (East China); Qingdao University; Zhejiang University of Technology; Qingdao University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Human–machine interaction (HMI) allows the transfer of human intent to the robot and the collection of feedback from the robot. Human perception of the outside world is a direct response to human brain training, but low-level perception movements of robots are more complex than advanced reason. In the study, we designed a self-powered electronic skin (SPES) based on a piezoelectric nanogenerator (PENG). SPES shows a good piezoelectric effect and certain mechanical flexibility and can realize gesture recognition and tracking by sensing external pressure stimulation in HMI. Through the feedback control of the closed-loop system, the equivalent behavior trigger of the real intelligent robotic capacitive touch sensors (CATS) and SPES can be realized. SPES and Robot Hall Rotary Position Sensor (HRPS) have small perceptual errors, and remote signal feedback and behavior control of intelligent robots are realized by wireless transmission equipment, which is a greater advantage in a flexible environment. The proposed SPES tracking application in the HMI has great potential in the future artificial intelligence environment, the auxiliary equipment for people with disabilities, and the human–machine cooperation in a flexible environment.

KeyWords AITranslate

nanogenerator selfpowered electronic skin feedback control attitude tracking humanmachine synchronization
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01476

Chinese Library Classification Number:

Citation Information:

Human–machine interaction (HMI) allows the transfer of human intent to the robot and the collection of feedback from the robot. Human perception of the outside world is a direct response to human brain training, but low-level perception movements of robots are more complex than advanced reason. In the study, we designed a self-powered electronic skin (SPES) based on a piezoelectric nanogenerator (PENG). SPES shows a good piezoelectric effect and certain mechanical flexibility and can realize gesture recognition and tracking by sensing external pressure stimulation in HMI. Through the feedback control of the closed-loop system, the equivalent behavior trigger of the real intelligent robotic capacitive touch sensors (CATS) and SPES can be realized. SPES and Robot Hall Rotary Position Sensor (HRPS) have small perceptual errors, and remote signal feedback and behavior control of intelligent robots are realized by wireless transmission equipment, which is a greater advantage in a flexible environment. The proposed SPES tracking application in the HMI has great potential in the future artificial intelligence environment, the auxiliary equipment for people with disabilities, and the human–machine cooperation in a flexible environment.

quote

GB/T 7714-2015 [1] Ming Zhang, Wanli Wang, Guoting Xia, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01476.
MLA [1] Ming Zhang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01476.
APA [1] Ming Zhang, Wanli Wang, Guoting Xia, Licheng Wang, & Kai Wang. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01476
IEEE [1] Ming Zhang, Wanli Wang, Guoting Xia, Licheng Wang, and Kai Wang, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01476. keywords: {nanogenerator selfpowered electronic skin feedback control attitude tracking humanmachine synchronization}