daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Preparation and Properties of Self-Supported Ni3S2@NiMo-LDH Composite Electrocatalytic Material AITranslate

School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ni3S2@NiMo-LDH composite electrocatalytic material was prepared on a nickel foam substrate through hydrothermal method.The phase composition,microstructure,and electrocatalytic properties of the prepared electrocatalytic material were characterized using X-ray diffractometer(XRD),scanning electron microscope(SEM),and electrochemical workstation.The experimental exresults demonstrate that Ni-Mo-LDH nanospheres are successfully grown on the Ni3S2 nanosheet substrate,obtaining Ni3S2@NiMo-LDH composite electrocatalytic material.The Ni3S2@NiMo-LDH composite electrocatalytic material exhibits an overpotential of 84.7 mV for the hydrogen evolution reaction(HER)at a current density of 10 mA/cm2,and an overpotential of 270 mV for the oxygen evolution reaction(OER)at 20 mA/cm2.The overall water splitting voltage of Ni3S2@NiMo-LDH two-electrode system required at a current density of 150 mA/cm2 is 2.19 V.Compared to the individual Ni3S2 and NiMo-LDH materials,the Ni3S2@NiMo-LDH composite material exhibits superior electrocatalytic properties and excellent stability.

KeyWords AITranslate

hydrothermal method electrocatalytic material Ni3S2@NiMo-LDH HER OER water splitting
No data

Basic Information:

DOI:

Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]

Citation Information:

Ni3S2@NiMo-LDH composite electrocatalytic material was prepared on a nickel foam substrate through hydrothermal method.The phase composition,microstructure,and electrocatalytic properties of the prepared electrocatalytic material were characterized using X-ray diffractometer(XRD),scanning electron microscope(SEM),and electrochemical workstation.The experimental exresults demonstrate that Ni-Mo-LDH nanospheres are successfully grown on the Ni3S2 nanosheet substrate,obtaining Ni3S2@NiMo-LDH composite electrocatalytic material.The Ni3S2@NiMo-LDH composite electrocatalytic material exhibits an overpotential of 84.7 mV for the hydrogen evolution reaction(HER)at a current density of 10 mA/cm2,and an overpotential of 270 mV for the oxygen evolution reaction(OER)at 20 mA/cm2.The overall water splitting voltage of Ni3S2@NiMo-LDH two-electrode system required at a current density of 150 mA/cm2 is 2.19 V.Compared to the individual Ni3S2 and NiMo-LDH materials,the Ni3S2@NiMo-LDH composite material exhibits superior electrocatalytic properties and excellent stability.

quote

GB/T 7714-2015 [1] LIU Xin-yu, KANG Xin, XIANG Jun, et al. Study on Preparation and Properties of Self-Supported Ni3S2@NiMo-LDH Composite Electrocatalytic Material[J]. Rare Metals and Cemented Carbides, 2025(5): 138-144.
MLA [1] LIU Xin-yu, et al., "Study on Preparation and Properties of Self-Supported Ni3S2@NiMo-LDH Composite Electrocatalytic Material." Rare Metals and Cemented Carbides, no. 5, 2025, pp. 138-144.
APA [1] LIU Xin-yu, KANG Xin, XIANG Jun, MA Dong-mei, LI Wei, HUANG Sheng-ling, & HUANG Yu-duo. (2025). Study on Preparation and Properties of Self-Supported Ni3S2@NiMo-LDH Composite Electrocatalytic Material. Rare Metals and Cemented Carbides(5), 138-144.
IEEE [1] LIU Xin-yu, KANG Xin, XIANG Jun, MA Dong-mei, LI Wei, HUANG Sheng-ling, and HUANG Yu-duo, "Study on Preparation and Properties of Self-Supported Ni3S2@NiMo-LDH Composite Electrocatalytic Material," Rare Metals and Cemented Carbides, no. 5, pp. 138-144, 2025. keywords: {hydrothermal method;electrocatalytic material;NiS@NiMo-LDH;HER;OER;water splitting}