daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Flexible Candlelight Organic LED on Mica Flexible Candlelight Organic LED on Mica AITranslate

National Tsing Hua University; National Tsing Hua University; National Tsing Hua University; National Tsing Hua University; National Yang Ming Chiao Tung University; National Tsing Hua University; National Yang Ming Chiao Tung University; National Tsing Hua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Candlelight-style, blue hazard-free light sources have been long desired in order to minimize the threats of blue emission on human health, artifacts, ecosystems, and night skies. Flexible light sources can enable numerous innovative products that are wearable, rollable, foldable, and portable. If also transparent, more applications including smart displays, lighting, signage, etc., can be implemented. However, current flexible lighting sources have issues like the use of environmentally unfriendly materials and poor lifetimes. Here, we show the fabrication and lifetime study of a candlelight-style organic light-emitting diode (LED) on high-flexibility, transparent mica that is 100% plastic-free. We found that the mica substrate coated with a transparent conductor survived a record-high bending curvature, i.e., 1/5 mm–1 and 50,000 bending cycles at a 7.5 mm bending radius. The candlelight organic LED fabricated thereon showed a good lifetime that is 83% of that on glass. The blue light-less emission permits at 100 lx an exposure limit of 47,000 s, while the exposure limit is 320 s for a cold-white counterpart; upon exposure at night for 1.5 h, it suppresses 1.6% melatonin, while 30% melatonin is suppressed for the cold-white counterpart. Our results demonstrate how blue hazard-free lighting sources are fabricated on eco-friendly mica that is highly flexible, and the resultant device showed a lifetime approaching that on glass due to its high resistance against moisture and oxygen penetration. The findings suggest that mica can be a good candidate for flexible transparent devices. We expect that these could bring up opportunities to promote omnifriendly lighting applications with a higher degree of design flexibility.

KeyWords AITranslate

blue hazardfree candlelightstyle flexible mica MPE MSS organic LED
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00123

Chinese Library Classification Number:

Citation Information:

Candlelight-style, blue hazard-free light sources have been long desired in order to minimize the threats of blue emission on human health, artifacts, ecosystems, and night skies. Flexible light sources can enable numerous innovative products that are wearable, rollable, foldable, and portable. If also transparent, more applications including smart displays, lighting, signage, etc., can be implemented. However, current flexible lighting sources have issues like the use of environmentally unfriendly materials and poor lifetimes. Here, we show the fabrication and lifetime study of a candlelight-style organic light-emitting diode (LED) on high-flexibility, transparent mica that is 100% plastic-free. We found that the mica substrate coated with a transparent conductor survived a record-high bending curvature, i.e., 1/5 mm–1 and 50,000 bending cycles at a 7.5 mm bending radius. The candlelight organic LED fabricated thereon showed a good lifetime that is 83% of that on glass. The blue light-less emission permits at 100 lx an exposure limit of 47,000 s, while the exposure limit is 320 s for a cold-white counterpart; upon exposure at night for 1.5 h, it suppresses 1.6% melatonin, while 30% melatonin is suppressed for the cold-white counterpart. Our results demonstrate how blue hazard-free lighting sources are fabricated on eco-friendly mica that is highly flexible, and the resultant device showed a lifetime approaching that on glass due to its high resistance against moisture and oxygen penetration. The findings suggest that mica can be a good candidate for flexible transparent devices. We expect that these could bring up opportunities to promote omnifriendly lighting applications with a higher degree of design flexibility.

quote

GB/T 7714-2015 [1] TunHao Chen, HaoJen Chen, ChingYu Weng, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00123.
MLA [1] TunHao Chen, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00123.
APA [1] TunHao Chen, HaoJen Chen, ChingYu Weng, FengRong Chen, DeShiang Liou, SunZen Chen, YingHao Chu, & JwoHuei Jou. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00123
IEEE [1] TunHao Chen, HaoJen Chen, ChingYu Weng, FengRong Chen, DeShiang Liou, SunZen Chen, YingHao Chu, and JwoHuei Jou, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00123. keywords: {blue hazardfree candlelightstyle flexible mica MPE MSS organic LED}