Ultra-fast uranium adsorption with phosphorylated tungsten disulfide nanosheets via sulfur defects AITranslate

National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing;National Key Laboratory of Uranium Resources Exploration-Mining and Nuclear Remote Sensing
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Rapid adsorption of radioactive substances is of great significance in emergency situations.A novel approach combining S-defect introduction and in situ phosphorization was employed to synthesize phosphorized WS2(WS2-PO4)for ultra-efficient uranium extraction.At an initial U(VI)concentration of 50 mg·L-1,the adsorption of U(VI)by WS2-PO4 nanosheets exceeds77%within just 1 min,with high selectivity(SU=78.7%)and good adsorption capacity of 268.82 mg·g-1.The phosphate groups have grown on the S defects and taken part in U(VI)extraction through surface complexation,leading to fast,reusable,and highly selective uranium adsorption,showing great potential in emergency treatment of radioactive nuclear wastewater.

KeyWords AITranslate

TUNGSTEN PHOSPHORYLATION URANIUM DEFECTS ADSORPTION
No data

Basic Information:

DOI:

Chinese Library Classification Number:X771[环境科学与工程—环境工程];TQ424[化学工程]

Citation Information:

Rapid adsorption of radioactive substances is of great significance in emergency situations.A novel approach combining S-defect introduction and in situ phosphorization was employed to synthesize phosphorized WS2(WS2-PO4)for ultra-efficient uranium extraction.At an initial U(VI)concentration of 50 mg·L-1,the adsorption of U(VI)by WS2-PO4 nanosheets exceeds77%within just 1 min,with high selectivity(SU=78.7%)and good adsorption capacity of 268.82 mg·g-1.The phosphate groups have grown on the S defects and taken part in U(VI)extraction through surface complexation,leading to fast,reusable,and highly selective uranium adsorption,showing great potential in emergency treatment of radioactive nuclear wastewater.

quote

GB/T 7714-2015 [1] Yuan-Ping Jiang, Guo-Hang He, Jin-Cao Chen, et al. Tungsten, 2025(4): 876-886.
MLA [1] Yuan-Ping Jiang, et al., Tungsten, no. 4, 2025, pp. 876-886.
APA [1] Yuan-Ping Jiang, Guo-Hang He, Jin-Cao Chen, Jia-Rui Zhou, Xing-Fang Yu, Long-Xu Wang, Xin Zeng, Jiang-Chen Liu, Jia-Jian Yang, Chong Lin, Xiao-Yu Hao, Zuo-Jia Li, Yun-Xiu Zhang, Zhi-Bin Zhang, & Yun-Hai Liu. (2025). Tungsten(4), 876-886.
IEEE [1] Yuan-Ping Jiang, Guo-Hang He, Jin-Cao Chen, Jia-Rui Zhou, Xing-Fang Yu, Long-Xu Wang, Xin Zeng, Jiang-Chen Liu, Jia-Jian Yang, Chong Lin, Xiao-Yu Hao, Zuo-Jia Li, Yun-Xiu Zhang, Zhi-Bin Zhang, and Yun-Hai Liu, Tungsten, no. 4, pp. 876-886, 2025.