Process for Improvement of Ta Wire Property AITranslate
Abstract AITranslate
Based on the traditional technology,large improvement is made on the key operations of small-diameter Ta wire,focusing on the elimination of the problems in Ta wire produced by original technology,such as high O_2 content;low tensile strength,poor surface quality,large tolerance,low resistance against partial O_2 brittleness.The new technology has resulted in better integral properties of Ta wire and increase of recovery by 5%.The product is qualified enough for export purpose.
KeyWords AITranslate
1李学芳.钽的近几年应用动态[J].钽铌工业进展,2001,72(1):19-19.
2曹寒松.提高细径钽丝抗脆性的研究[J].稀有金属与硬质合金,1998,26(3):16-21. 被引量:1
1万庆峰,王德志,赵兵.掺杂与钽丝毛刺的关系研究[J].稀有金属,2008,32(3):381-386. 被引量:1
2李仲香,包玺芳,张健康.实验设计方法改进钽丝用钽粉的酸洗工艺[J].宁夏工程技术,2010,9(3):238-241. 被引量:1
3陈国庆,张秉刚,庄园,邓冰辉,冯吉才.钽与不锈钢电子束焊接接头组织及性能(英文)[J].稀有金属材料与工程,2013,42(5):914-918. 被引量:10
4包玺芳,解永旭,王晖晖.采用DOE实验设计方法改进电容器级铌粉酸洗工艺[J].粉末冶金技术,2017,35(5):371-377. 被引量:1
5包玺芳,解永旭.改善钽丝直线度的研究[J].粉末冶金技术,2020,38(5):340-343.
1陈国庆,张秉刚,赵宇星,冯吉才.难熔金属与钢异种材料焊接研究现状[J].焊接,2014(7):21-25. 被引量:4
2王亚荣,张勇智,余洋,许超.镀层金属对钒合金与不锈钢电子束焊接头组织与性能的影响[J].稀有金属材料与工程,2015,44(4):875-880. 被引量:3
3赵连风,易丹青,刘欢,王琪,王斌.M42高速钢/X32弹簧钢电子束焊接温度场的数值模拟与实验研究[J].粉末冶金材料科学与工程,2015,20(4):513-521. 被引量:3
4张洪刚,雒国清.大球磨机在高压钽锭上的应用[J].世界有色金属,2016,0(9):141-141.
5杨全虎,翟秋亚,徐锦锋,纪腾飞,叶建林.Ta1与0Cr18Ni9薄板的储能焊试验[J].焊接学报,2019,40(9):116-121. 被引量:3
6陈燕飞,赖华生,朱政强,文小强,袁德林,王玉香.钨极氩弧搭接焊钽片接头的显微组织[J].机械工程材料,2020,44(9):31-35.
7翟秋亚,刘帅宾,杨全虎,叶建林,徐锦锋.Ta1/0Cr18Ni9薄板储能焊熔核高熵化机理[J].焊接学报,2020,41(8):79-84. 被引量:3
8翟秋亚,刘帅宾,杨全虎,叶建林,徐锦锋.Ta1/Ta8Ni30Cr20Cu42/0Cr18Ni9储能焊接头组织与性能[J].焊接学报,2020,41(10):60-64. 被引量:3
9陈燕飞,张金祥,周吉学,朱政强.钽的焊接技术研究进展[J].电焊机,2021,51(1):37-41. 被引量:1
10刘泽程,王国伟,肖祥友,刘锋.选择性激光熔化镍基高温合金的工艺优化[J].粉末冶金技术,2021,39(1):81-88. 被引量:2
1詹艳然,吴建国.细径钽丝轧制过程的数值模拟[J].塑性工程学报,2005(z1):168-171.
2万庆峰,田苗,陈林,赵兵,马跃忠.掺杂元素Ge和Ce及掺杂量对钽丝组织和性能的影响[J].材料热处理学报,2013,34(9):127-131. 被引量:2
3曹寒松.提高细径钽丝抗脆性的研究[J].稀有金属与硬质合金,1998,26(3):16-21. 被引量:1
4静恩志,杨义纲.液锌抗氧素在热镀锌锅上的应用[J].金属制品,2005,31(2):32-32.
5周龙江,张亚明.铝,硅共渗提高γ/γ′—α—Mo定向共晶合金抗氧…[J].中国腐蚀与防护学报,1997,17(A05):475-479.
6吴明,陈丽.等离子喷涂热障涂层抗氧化性能研究[J].石油化工高等学校学报,2004,17(4):69-71. 被引量:2
7张澜庭,吴建生,邱国华.Ti_3Al基合金高温氧化行为的原位X射线衍射研究[J].稀有金属材料与工程,1997,26(2):23-26. 被引量:6
8YKM电火花加工液[J].合成润滑材料,2005,32(1):21-21.
9陆峰,李洪建,郭睿,唐力.一种新型缓蚀剂对A3钢的缓蚀性能研究[J].重庆科技学院学报:自然科学版,2010,12(3):110-112. 被引量:5
10成崇远,李子存,宋世远,张杰,蒲改霞,杨靖,张晶.精密钢管拉拔油的研制[J].润滑与密封,2003,28(3):78-78.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]
Citation Information:
Based on the traditional technology,large improvement is made on the key operations of small-diameter Ta wire,focusing on the elimination of the problems in Ta wire produced by original technology,such as high O_2 content;low tensile strength,poor surface quality,large tolerance,low resistance against partial O_2 brittleness.The new technology has resulted in better integral properties of Ta wire and increase of recovery by 5%.The product is qualified enough for export purpose.
quote
| GB/T 7714-2015 | [1] CAO Han-song. Process for Improvement of Ta Wire Property[J]. Rare Metals and Cemented Carbides, 2002(2): 28-32. |
| MLA | [1] CAO Han-song. "Process for Improvement of Ta Wire Property." Rare Metals and Cemented Carbides, no. 2, 2002, pp. 28-32. |
| APA | [1] CAO Han-song. (2002). Process for Improvement of Ta Wire Property. Rare Metals and Cemented Carbides(2), 28-32. |
| IEEE | [1] CAO Han-song, "Process for Improvement of Ta Wire Property," Rare Metals and Cemented Carbides, no. 2, pp. 28-32, 2002. keywords: {small-diameter Ta wire;integral properties;doped} |