Flexible CNT-MXene-CNT Film with Low Surface Conductance for High- and Low-Power Electromagnetic Absorption Protection Flexible CNT-MXene-CNT Film with Low Surface Conductance for High- and Low-Power Electromagnetic Absorption Protection AITranslate
Abstract AITranslate
High absorption performance terahertz (THz) and GHz absorbers with low surface conductance are urgently indispensable in the application of military electromagnetic protection and multiband communication. Herein, cost-effective approaches of modified grafting and hot-pressing molding methods are proposed to construct CNT-MXene-CNT films based on a modified methyl vinyl silicone rubber (MVSR). The resultant 3 mm CNT-1.1-MXene-1.9-CNT-1.1 sample exhibits average electromagnetic interference shielding effectiveness (EMI SE) of about 29.2 dB in the range of 2–12.5 GHz and favorable EMI SE of 48.2 dB within 0.1–2.2 THz. In addition, the optimized sample also obtains excellent EMI SE of about 31.8 and 41.2 dB under the high-power test conditions in the GHz and THz bands. Besides, the CNT-1.1-MXene-1.9-CNT-1.1 sample possesses only about 1.5% overall loading content with a low surface conductivity of 2.3 μS/m. The as-prepared absorber with a low surface conductance demonstrates enormous potential in future military and civilian applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c01285
Chinese Library Classification Number:
Citation Information:
High absorption performance terahertz (THz) and GHz absorbers with low surface conductance are urgently indispensable in the application of military electromagnetic protection and multiband communication. Herein, cost-effective approaches of modified grafting and hot-pressing molding methods are proposed to construct CNT-MXene-CNT films based on a modified methyl vinyl silicone rubber (MVSR). The resultant 3 mm CNT-1.1-MXene-1.9-CNT-1.1 sample exhibits average electromagnetic interference shielding effectiveness (EMI SE) of about 29.2 dB in the range of 2–12.5 GHz and favorable EMI SE of 48.2 dB within 0.1–2.2 THz. In addition, the optimized sample also obtains excellent EMI SE of about 31.8 and 41.2 dB under the high-power test conditions in the GHz and THz bands. Besides, the CNT-1.1-MXene-1.9-CNT-1.1 sample possesses only about 1.5% overall loading content with a low surface conductivity of 2.3 μS/m. The as-prepared absorber with a low surface conductance demonstrates enormous potential in future military and civilian applications.
quote
| GB/T 7714-2015 | [1] Yunbo Guo, Yu Bai, Yinxiang Lu. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01285. |
| MLA | [1] Yunbo Guo, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01285. |
| APA | [1] Yunbo Guo, Yu Bai, & Yinxiang Lu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01285 |
| IEEE | [1] Yunbo Guo, Yu Bai, and Yinxiang Lu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01285. keywords: {CNT MXene electromagnetic interference absorption terahertz low surface conductance} |