Efficient Narrow-Band Green Light-Emitting Hybrid Halides for Wide Color Gamut Display Efficient Narrow-Band Green Light-Emitting Hybrid Halides for Wide Color Gamut Display AITranslate
Abstract AITranslate
Phosphors with narrow-band emission are in great demand for liquid crystal display backlighting applications. In this work, four zero-dimensional Mn2+-based organic–inorganic metal halides (OIMHs), (C13H26N)3MnBr4·Br, (C13H26N)2MnCl4, and (C7H18N)2MnX4 (X = Cl, Br), were synthesized, and their crystal structures were solved. Under blue-light excitation, all of the materials exhibited bright narrow-band green luminescence centered at 515–525 nm with high photoluminescence quantum yields (PLQYs). Significantly, (C13H26N)3MnBr4·Br and (C13H26N)2MnCl4 exhibited small full width at half-maximum (FWHM) values of 43 and 48 nm with PLQYs of 77.8 and 79.3% at room temperature, respectively. Compared with the reported luminescent OIMHs, ultrahigh thermal quenching temperatures were observed, and at 420 K, emission intensities of (C13H26N)3MnBr4·Br and (C13H26N)2MnCl4, remained 82.7 and 64.2% of those at room temperature, respectively. The rigid environment provided by the C13H26N+ cation has a strong confinement effect on the [MnX4]2– tetrahedra, leading to a narrower FWHM and higher thermal quenching temperature. Finally, (C13H26N)3MnBr4·Br was combined with commercial phosphors to fabricate light-emitting diodes (LEDs) with a wide color gamut of up to 113% NTSC (National Television System Committee). This work provides a reference for designing the OIMHs for liquid crystal display LEDs by tuning the organic cations.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00705
Chinese Library Classification Number:
Citation Information:
Phosphors with narrow-band emission are in great demand for liquid crystal display backlighting applications. In this work, four zero-dimensional Mn2+-based organic–inorganic metal halides (OIMHs), (C13H26N)3MnBr4·Br, (C13H26N)2MnCl4, and (C7H18N)2MnX4 (X = Cl, Br), were synthesized, and their crystal structures were solved. Under blue-light excitation, all of the materials exhibited bright narrow-band green luminescence centered at 515–525 nm with high photoluminescence quantum yields (PLQYs). Significantly, (C13H26N)3MnBr4·Br and (C13H26N)2MnCl4 exhibited small full width at half-maximum (FWHM) values of 43 and 48 nm with PLQYs of 77.8 and 79.3% at room temperature, respectively. Compared with the reported luminescent OIMHs, ultrahigh thermal quenching temperatures were observed, and at 420 K, emission intensities of (C13H26N)3MnBr4·Br and (C13H26N)2MnCl4, remained 82.7 and 64.2% of those at room temperature, respectively. The rigid environment provided by the C13H26N+ cation has a strong confinement effect on the [MnX4]2– tetrahedra, leading to a narrower FWHM and higher thermal quenching temperature. Finally, (C13H26N)3MnBr4·Br was combined with commercial phosphors to fabricate light-emitting diodes (LEDs) with a wide color gamut of up to 113% NTSC (National Television System Committee). This work provides a reference for designing the OIMHs for liquid crystal display LEDs by tuning the organic cations.
quote
| GB/T 7714-2015 | [1] Na Wang, Yan Xiong, Kunjie Liu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00705. |
| MLA | [1] Na Wang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00705. |
| APA | [1] Na Wang, Yan Xiong, Kunjie Liu, Shihui He, Jindong Cao, Xusheng Zhang, Jing Zhao, & Quanlin Liu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00705 |
| IEEE | [1] Na Wang, Yan Xiong, Kunjie Liu, Shihui He, Jindong Cao, Xusheng Zhang, Jing Zhao, and Quanlin Liu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00705. keywords: {organic−inorganic hybrid metal halides narrowband green emission high photoluminescence quantum yields excellent thermalShow More} |