X-ray Absorption Fine Structural Study of Atomic Structures and Chemical States of Dopants in 4H-SiC(0001) X-ray Absorption Fine Structural Study of Atomic Structures and Chemical States of Dopants in 4H-SiC(0001) AITranslate

Kyushu University; Kyushu University; Kyushu University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The atomic structures and chemical states of active and inactive dopant sites in n-type and p-type 4H-SiC(0001) substrates have been investigated by X-ray absorption near edge structure (XANES) and photoelectron spectroscopy (PES). In N atom-doped n-type 4H-SiC(0001), the PES results indicated that a N–C species was formed near the surface. XANES simulations showed that SiNx and N–C species were attributed to active and inactive dopant states, respectively. Angle-resolved XANES measurements showed that the N–C species acted as an inactive dopant site in N-doped 4H-SiC(0001). In Al-doped p-type 4H-SiC, PES analysis revealed that a single chemical state was present at the Al-doped 4H-SiC. The simulated XANES spectra showed that the Si site in 4H-SiC(0001) was replaced by an Al dopant atom, which was the active dopant site. Furthermore, relaxation of the local structure around the Al dopant in Al-doped 4H-SiC(0001) was observed due to bond stretching.

KeyWords AITranslate

SiC Ndoped SiC Aldoped SiC active and inactive dopant
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00546

Chinese Library Classification Number:

Citation Information:

The atomic structures and chemical states of active and inactive dopant sites in n-type and p-type 4H-SiC(0001) substrates have been investigated by X-ray absorption near edge structure (XANES) and photoelectron spectroscopy (PES). In N atom-doped n-type 4H-SiC(0001), the PES results indicated that a N–C species was formed near the surface. XANES simulations showed that SiNx and N–C species were attributed to active and inactive dopant states, respectively. Angle-resolved XANES measurements showed that the N–C species acted as an inactive dopant site in N-doped 4H-SiC(0001). In Al-doped p-type 4H-SiC, PES analysis revealed that a single chemical state was present at the Al-doped 4H-SiC. The simulated XANES spectra showed that the Si site in 4H-SiC(0001) was replaced by an Al dopant atom, which was the active dopant site. Furthermore, relaxation of the local structure around the Al dopant in Al-doped 4H-SiC(0001) was observed due to bond stretching.

quote

GB/T 7714-2015 [1] Yuhua Tsai, Jingmin Tang, Yoshiyuki Yamashita. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00546.
MLA [1] Yuhua Tsai, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00546.
APA [1] Yuhua Tsai, Jingmin Tang, & Yoshiyuki Yamashita. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00546
IEEE [1] Yuhua Tsai, Jingmin Tang, and Yoshiyuki Yamashita, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00546. keywords: {SiC Ndoped SiC Aldoped SiC active and inactive dopant}