Study of Preparation of Molybdenum Disulfide Nanoparticlesby Thermal Decomposition AITranslate

School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University;School of Materials and Metallurgical of Northeast University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Molybdenum disulfide nanoparticles is prepared by thermal decomposition of ammonium tetrathiomolybdate.The morphology, composition and structure of the product is tested by TEM,SEM,XRD and ED.Results showed that the resultant dark-gray molybdenum disulfide nanoparticles have average diameter less than 100 nm.The product is hexagonal lattice,a=0.316 nm,c=1.229 nm,it is quite pure,almost free of impurities from comparison of X-ray diffraction pattern with JCPDS.ED analysis also showed that nanoparticles were highly-crystallized multi-crystals,with continuous and clear diffraction ring at surface such as (0004), (0110) and (0112) in conformance with XRD analysis results.Discussion is made on the factors affecting the formation of molybdenum disulfide powder such as the reaction temperature,duration,the material layer thickness,carrier gas flowrate,the reaction material.

KeyWords AITranslate

molybdenum disulfide nano-powder thermal decomposition characterization affecting factors

1曹茂盛.超微颗粒制备科学与技术[M].哈尔滨:哈尔滨工业大学出版社,1995..

2田中隆夫.铁基氮化物超微粒子的合成及其特性[J].日本化学会志,1984,(6):930-930.

3张文钲.纳米级二硫化钼的研发现状[J].中国钼业,2000,24(5):23-26. 被引量:16

4Wie-Hinpan,et al.Facile syntheses of new molybdenum and tungsten sulfide complexes,structure of Mo3O2-9[J].Inorganic Chemistry,1983, 22: 672.

5Prasad T P,et al.Thermal decomposition of (NH4)2MoO2S2,(NH4)2MoS4,(NH4)2WO2S2 and (NH4)2WS[J].J Inorg Nucl Chem,1973,35:1895.

1何杰,管翠诗,安长华,王宗贤.过渡金属硫化物纳米粒子制备技术研究进展[J].工业催化,2007,15(4):6-10. 被引量:6

2徐志昌,张萍.MoS_2纳米材料化学合成工艺流程的研究[J].中国钼业,2009,33(6):11-25. 被引量:2

3刘前明,肖连生,曾理,龚柏凡.水合肼直接还原硫代钼酸铵晶体制备超细二硫化钼[J].中国钼业,2012,36(2):35-38. 被引量:2

4白鸽玲,吴壮志.二硫化钼纳米球的制备及其摩擦性能研究[J].润滑与密封,2013,38(4):93-96. 被引量:17

5侯锁霞,霍英杰,李勇帅,吴超,张舵,张好强.MoS_2的合成及其在润滑领域应用研究进展[J].兵器材料科学与工程,2018,41(1):123-126. 被引量:3

1李大成,周新文,唐丽霞.二硫化钼生产制备技术及应用分析[J].中国钼业,2008,32(3):8-11. 被引量:16

2徐志昌,张萍.MoS_2纳米材料化学合成工艺流程的研究[J].中国钼业,2009,33(6):11-25. 被引量:2

3龙曾成,伍秋美,杨海林,阮建明.溶剂热法合成CoS纳米晶及其表征[J].粉末冶金材料科学与工程,2011,16(6):886-891. 被引量:3

4张亨.二硫化钼的性质、生产和应用[J].中国钼业,2014,38(1):7-10. 被引量:7

5李斌,谢凤,张蒙蒙,李磊.纳米二硫化钼作为润滑油添加剂的摩擦学性能研究[J].润滑与密封,2014,39(9):91-95. 被引量:19

6阎鑫,闫从祥,赵坤,艾涛,苏兴华,赵鹏.纳米二硫化钼氧化石墨烯复合材料的制备及催化性能研究[J].中国钼业,2014,38(6):22-25. 被引量:3

7马少华.油溶性硫化锌纳米微粒的制备及抗磨性能评价[J].当代化工,2015,44(3):458-460.

8张亨.纳米二硫化钼的制备及性质研究进展[J].中国钼业,2015,39(3):5-9. 被引量:9

9施凯烽,谢凤.二硫化钼润滑添加剂摩擦学性能研究现状[J].山东化工,2017,46(4):55-56. 被引量:4

10霍英杰,侯锁霞,张好强,吴超,张舵.纳米二硫化钼的水热法可控制备及极压性能研究[J].润滑与密封,2017,42(9):107-110. 被引量:6

1马江虹,翟玉春.热分解法制备WS_2纳米粉体的研究[J].材料导报,2004,18(5):97-99.

2金太权,雷军,金恩姬.γ-Fe_2O_3溅射磁膜的制作[J].真空科学与技术学报,1991,0(3):186-190.

3章高潮,王犁.流化床速冻装置的特性分析及应用[J].制冷学报,1992,14(4):41-44.

4黄丽,徐定宇,徐从鹏.聚甲醛钢背铜塑三层结构复合材料的加工工艺与性能研究[J].复合材料学报,1999,16(3):30-33. 被引量:2

5卞波,张庶元,吴自勤.a-Si∶H/Au/a-Si∶H膜的退火行为[J].电子显微学报,1993,12(2):156-156.

6蒋剑良.MEMS多层悬梁微执行器的电-热分析模型研究[J].北京理工大学学报,2005,25(6):512-516.

7段兴凯,江跃珍.真空电弧等离子体合成(Bi_xSb_(1-x))_2Te_3纳米粉末材料[J].稀有金属,2011,35(3):394-397. 被引量:6

8徐超,孙凤莲,秦优琼,孟工戈.金刚石与硬质合金钎焊接头应力场分析[J].焊接学报,2003,24(2):47-50. 被引量:15

9韩俊鹤,欧慧灵,廖鹏,王长顺,顾玉宗,余保龙.表面修饰的Bi_2O_3纳米微粒的光学特性[J].河南大学学报:自然科学版,2001,31(3):14-16. 被引量:3

10李延民,王海鹏,洪祯.轮胎辊与锥辊立磨粉磨过程力学分析[J].中国粉体技术,2016,22(6):90-94. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]

Citation Information:

Molybdenum disulfide nanoparticles is prepared by thermal decomposition of ammonium tetrathiomolybdate.The morphology, composition and structure of the product is tested by TEM,SEM,XRD and ED.Results showed that the resultant dark-gray molybdenum disulfide nanoparticles have average diameter less than 100 nm.The product is hexagonal lattice,a=0.316 nm,c=1.229 nm,it is quite pure,almost free of impurities from comparison of X-ray diffraction pattern with JCPDS.ED analysis also showed that nanoparticles were highly-crystallized multi-crystals,with continuous and clear diffraction ring at surface such as (0004), (0110) and (0112) in conformance with XRD analysis results.Discussion is made on the factors affecting the formation of molybdenum disulfide powder such as the reaction temperature,duration,the material layer thickness,carrier gas flowrate,the reaction material.

quote

GB/T 7714-2015 [1] MA Jiang-hong, DI Yu-chun, TIAN Yan-wen. Study of Preparation of Molybdenum Disulfide Nanoparticlesby Thermal Decomposition[J]. Rare Metals and Cemented Carbides, 2004(3): 1-4.
MLA [1] MA Jiang-hong, et al., "Study of Preparation of Molybdenum Disulfide Nanoparticlesby Thermal Decomposition." Rare Metals and Cemented Carbides, no. 3, 2004, pp. 1-4.
APA [1] MA Jiang-hong, DI Yu-chun, & TIAN Yan-wen. (2004). Study of Preparation of Molybdenum Disulfide Nanoparticlesby Thermal Decomposition. Rare Metals and Cemented Carbides(3), 1-4.
IEEE [1] MA Jiang-hong, DI Yu-chun, and TIAN Yan-wen, "Study of Preparation of Molybdenum Disulfide Nanoparticlesby Thermal Decomposition," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2004. keywords: {molybdenum disulfide nano-powder;thermal decomposition;characterization;affecting factors}