Technical Improvement for Recovery of Tin,Antimony and Bismuth by Reverberatory Furnace AITranslate

CINF Engineering Co.,Ltd.;CINF Engineering Co.,Ltd.;CINF Engineering Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Three rounds of technological improvement were carried out on the reverberatory furnace smelting process for the recovery of tin, antimony and bismuth.The main measures were employed of adding water-cooled flue, replacing solid fuels with gas fuels and increasing oxygen enriched smelting.The technological improvement has a significant effect and promotes the development of reverberatory furnace smelting technology in the direction of environmental protection and energy saving, making a demonstration for the industry to promote the upgrading of reverberatory furnace smelting technology.

KeyWords AITranslate

reverberatory furnace smelting tin antimony and bismuth recovery technical improvement

1刘树景.铜精炼反射炉的生产和实践[J].资源再生,2010(12):60-62. 被引量:4

2陈宝成.内蒙古某冶炼厂反射炉炼锡生产实践[J].有色矿冶,2019,35(1):35-38. 被引量:1

3李良东,刘斌莲,王明辉,王选国.铅浮渣反射炉改进实践[J].有色矿冶,2013,29(3):26-28. 被引量:1

4牛勤学,付国秀.铜浮渣反射炉结构改造实践探索[J].湖南有色金属,2011,27(4):35-36. 被引量:4

5朱文平.铋熔炼反射炉进出料系统结构优化研究[J].湖南有色金属,2014,30(1):37-39. 被引量:3

6张霞,童莉葛,王立,刘传平.富氧燃烧技术的应用现状分析[J].冶金能源,2007,26(6):41-44. 被引量:27

1贾华平.论坛寄语[J].中国水泥,2021(3):74-74.

2模块化超低氮蒸汽热源机[J].上海节能,2021(4):436-437.

3杨奕兵,周剑,刘亚洲.电弧炉水冷烟道汽化冷却技术改造[J].现代冶金,2020,48(4):40-42.

4王斌,曾万川,华志宇.高钛渣直流电炉煤气干法冷却及净化系统设计要点[J].有色金属设计,2020,47(2):23-30.

5刘兴来.连续吹炼炉技术改造工业实践[J].冶金管理,2020(9):6-7.

6刘刚,彭叔森,王春霞,师超,刘光明.环保节能型发蓝工艺综合性实验教学的设计与实践[J].广州化工,2021,49(8):149-152. 被引量:1

7期刊征订[J].中国矿山工程,2021,50(2).

8蔡欣怡.中国古代青铜器艺术的简述[J].花溪,2021(9):0181-0181.

9潘权文,颜莹,李小武,王斌,张鹏,张哲峰.热处理对双真空冶炼AISI 4340钢显微组织和拉伸性能的影响[J].材料热处理学报,2021,42(4):87-95. 被引量:3

10王越,孙景晓,王现杰,辛丽莎,刘泉秀.微波消解-电感耦合等离子体原子发射光谱法测定铁矿石中硅和磷[J].冶金分析,2021,41(2):44-48. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TF806.22[冶金工程—有色金属冶金]

Citation Information:

Three rounds of technological improvement were carried out on the reverberatory furnace smelting process for the recovery of tin, antimony and bismuth.The main measures were employed of adding water-cooled flue, replacing solid fuels with gas fuels and increasing oxygen enriched smelting.The technological improvement has a significant effect and promotes the development of reverberatory furnace smelting technology in the direction of environmental protection and energy saving, making a demonstration for the industry to promote the upgrading of reverberatory furnace smelting technology.

quote

GB/T 7714-2015 [1] DONG Xiao-wei, WANG Heng-hui, ZHOU Xiao-yuan. Technical Improvement for Recovery of Tin,Antimony and Bismuth by Reverberatory Furnace[J]. Rare Metals and Cemented Carbides, 2021(2): 20-23.
MLA [1] DONG Xiao-wei, et al., "Technical Improvement for Recovery of Tin,Antimony and Bismuth by Reverberatory Furnace." Rare Metals and Cemented Carbides, no. 2, 2021, pp. 20-23.
APA [1] DONG Xiao-wei, WANG Heng-hui, & ZHOU Xiao-yuan. (2021). Technical Improvement for Recovery of Tin,Antimony and Bismuth by Reverberatory Furnace. Rare Metals and Cemented Carbides(2), 20-23.
IEEE [1] DONG Xiao-wei, WANG Heng-hui, and ZHOU Xiao-yuan, "Technical Improvement for Recovery of Tin,Antimony and Bismuth by Reverberatory Furnace," Rare Metals and Cemented Carbides, no. 2, pp. 20-23, 2021. keywords: {reverberatory furnace;smelting;tin;antimony and bismuth;recovery;technical improvement}