Post-Process-Functionalized Catalytic Electrospun and 2D-Printed Structures for Wolf–Lamb-Type Catalysis AITranslate
Abstract AITranslate
A process for preparing active, strong base and acid self-standing individual membranes and printed structures is established by electrospinning and two-dimensional (2D) printing of the corresponding polymeric base and polymeric acid on a neutral plastic substrate. The active polymeric acid and strong base used in this work were (poly(styrene-co-styrene sulfonic acid-co-methacryloyl benzophenone)) and poly(styrene-co-4-vinylbenzylamine-co-N-(4-benzoylphenyl)acrylamide), respectively. The active acid–base printed structures and membranes were compared for their activity in a standard two-step acid-catalyzed deacetalization reaction of dimethoxybenzyl acetal to benzaldehyde followed by a base-catalyzed Knoevenagel condensation with ethyl cyanoacetate toward ethyl-2-cyano-3-phenyl acrylate reaction in one pot in different solvents. Both 2D-printed acid–base structures and electrospun membranes could be arranged in one pot to complete the two-step reaction without destroying each other’s activity. High conversions, fast reaction, and reusability make 2D-printed structures favorable in toluene over electrospun membranes. The kinetic parameters were also calculated to address the solvent’s influence and further strengthen the systems’ understanding and comparison.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01197
Chinese Library Classification Number:
Citation Information:
A process for preparing active, strong base and acid self-standing individual membranes and printed structures is established by electrospinning and two-dimensional (2D) printing of the corresponding polymeric base and polymeric acid on a neutral plastic substrate. The active polymeric acid and strong base used in this work were (poly(styrene-co-styrene sulfonic acid-co-methacryloyl benzophenone)) and poly(styrene-co-4-vinylbenzylamine-co-N-(4-benzoylphenyl)acrylamide), respectively. The active acid–base printed structures and membranes were compared for their activity in a standard two-step acid-catalyzed deacetalization reaction of dimethoxybenzyl acetal to benzaldehyde followed by a base-catalyzed Knoevenagel condensation with ethyl cyanoacetate toward ethyl-2-cyano-3-phenyl acrylate reaction in one pot in different solvents. Both 2D-printed acid–base structures and electrospun membranes could be arranged in one pot to complete the two-step reaction without destroying each other’s activity. High conversions, fast reaction, and reusability make 2D-printed structures favorable in toluene over electrospun membranes. The kinetic parameters were also calculated to address the solvent’s influence and further strengthen the systems’ understanding and comparison.
quote
| GB/T 7714-2015 | [1] Martin O. Pretscher, Gabriel Sitaru, Markus Dietel, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01197. |
| MLA | [1] Martin O. Pretscher, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01197. |
| APA | [1] Martin O. Pretscher, Gabriel Sitaru, Markus Dietel, Holger Schmalz, Stephan Gekle, & Seema Agarwal. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01197 |
| IEEE | [1] Martin O. Pretscher, Gabriel Sitaru, Markus Dietel, Holger Schmalz, Stephan Gekle, and Seema Agarwal, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01197. keywords: {catalysis;acid−base;one pot;electrospinning;3D printing} |