Ferroelectric Content-Addressable Memory Cells with IGZO Channel: Impact of Retention Degradation on the Multibit Operation Ferroelectric Content-Addressable Memory Cells with IGZO Channel: Impact of Retention Degradation on the Multibit Operation AITranslate
Abstract AITranslate
Indium gallium zinc oxide (IGZO)-based ferroelectric thin-film transistors (FeTFTs) are being vigorously investigated for being deployed in computing-in-memory (CIM) applications. Content-addressable memories (CAMs) are the quintessential example of CIM, which conduct a parallel search over a queue or stack to obtain the matched entries for a given input data. CAM cells offer the ability for massively parallel searches in a single clock cycle throughout an entire CAM array for the input query, thereby enabling pattern matching and searching functionality. Therefore, CAM cells are used extensively for pattern matching or search operations in data-centric computing. This paper investigates the impact of retention degradation on IGZO-based FeTFT on the multibit operation in content CAM cell applications. We propose a scalable multibit 1FeTFT-1T-based CAM cell composed of only one FeTFT and one transistor, thus significantly improving the density and energy efficiency compared with conventional complementary metal–oxide–semiconductor (CMOS)-based CAM. We successfully demonstrate the operations of our proposed CAM with storage and search by exploiting the multilevel states of the experimentally calibrated IGZO-based FeTFT devices. We also investigate the impact of retention degradation on the search operation. Our proposed IGZO-based 3-bit and 2-bit CAM cell shows 104 s and 106 s retention, respectively. The single-bit CAM cell shows lifelong (10 years) retention.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01357
Chinese Library Classification Number:
Citation Information:
Indium gallium zinc oxide (IGZO)-based ferroelectric thin-film transistors (FeTFTs) are being vigorously investigated for being deployed in computing-in-memory (CIM) applications. Content-addressable memories (CAMs) are the quintessential example of CIM, which conduct a parallel search over a queue or stack to obtain the matched entries for a given input data. CAM cells offer the ability for massively parallel searches in a single clock cycle throughout an entire CAM array for the input query, thereby enabling pattern matching and searching functionality. Therefore, CAM cells are used extensively for pattern matching or search operations in data-centric computing. This paper investigates the impact of retention degradation on IGZO-based FeTFT on the multibit operation in content CAM cell applications. We propose a scalable multibit 1FeTFT-1T-based CAM cell composed of only one FeTFT and one transistor, thus significantly improving the density and energy efficiency compared with conventional complementary metal–oxide–semiconductor (CMOS)-based CAM. We successfully demonstrate the operations of our proposed CAM with storage and search by exploiting the multilevel states of the experimentally calibrated IGZO-based FeTFT devices. We also investigate the impact of retention degradation on the search operation. Our proposed IGZO-based 3-bit and 2-bit CAM cell shows 104 s and 106 s retention, respectively. The single-bit CAM cell shows lifelong (10 years) retention.
quote
| GB/T 7714-2015 | [1] Masud Rana Sk, Sunanda Thunder, David Lehninger, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01357. |
| MLA | [1] Masud Rana Sk, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01357. |
| APA | [1] Masud Rana Sk, Sunanda Thunder, David Lehninger, Shawn Sanctis, Yannick Raffel, Maximilian Lederer, Michael P. M. Jank, Thomas Kämpfe, Sourav De, & Bhaswar Chakrabarti. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01357 |
| IEEE | [1] Masud Rana Sk, Sunanda Thunder, David Lehninger, Shawn Sanctis, Yannick Raffel, Maximilian Lederer, Michael P. M. Jank, Thomas Kämpfe, Sourav De, and Bhaswar Chakrabarti, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01357. keywords: {computinginmemory (CIM) contentaddressable memory (CAM) ferroelectric memory HZO IGZO FeTFT} |