daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on the Effect of Hot Rolling Finishing Temperature on the Properties of Beryllium Copper Alloy Plates AITranslate

Productivity Promotion Center of Ningxia Hui Autonomous Region
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The finishing temperature during hot rolling of beryllium bronze has significant impact on the microstructure and properties of beryllium copper alloy plates.Mechanical properties and microstructure of beryllium copper alloy plates with different hot rolling finishing temperatures subjected to identical subsequent cold rolling and heat treatment processes were analyzed by tensile property,hardness and electrical conductivity measurements,along with SEM and EDS.The corresponding variation trends were investigated.The results indicate that with increasing the hot rolling finishing temperature from 520℃to 620℃,the Vickers hardness,tensile strength,yield strength,elongation after fracture and elastic modulus of beryllium copper alloy plates gradually increase,while the electrical conductivity decreases.This is primarily due to the more severe grain boundary reactions and highβ-phase content in the beryllium copper alloy plates at lower hot rolling finishing temperature,leading to the deterioration of alloy properties.

KeyWords AITranslate

beryllium copper alloy hot rolling finishing temperature mechanical property microstructure
No data

Basic Information:

DOI:

Chinese Library Classification Number:TG389[金属学及工艺]

Citation Information:

The finishing temperature during hot rolling of beryllium bronze has significant impact on the microstructure and properties of beryllium copper alloy plates.Mechanical properties and microstructure of beryllium copper alloy plates with different hot rolling finishing temperatures subjected to identical subsequent cold rolling and heat treatment processes were analyzed by tensile property,hardness and electrical conductivity measurements,along with SEM and EDS.The corresponding variation trends were investigated.The results indicate that with increasing the hot rolling finishing temperature from 520℃to 620℃,the Vickers hardness,tensile strength,yield strength,elongation after fracture and elastic modulus of beryllium copper alloy plates gradually increase,while the electrical conductivity decreases.This is primarily due to the more severe grain boundary reactions and highβ-phase content in the beryllium copper alloy plates at lower hot rolling finishing temperature,leading to the deterioration of alloy properties.

quote

GB/T 7714-2015 [1] HAN Lei. Study on the Effect of Hot Rolling Finishing Temperature on the Properties of Beryllium Copper Alloy Plates[J]. Rare Metals and Cemented Carbides, 2026(1): 128-133.
MLA [1] HAN Lei. "Study on the Effect of Hot Rolling Finishing Temperature on the Properties of Beryllium Copper Alloy Plates." Rare Metals and Cemented Carbides, no. 1, 2026, pp. 128-133.
APA [1] HAN Lei. (2026). Study on the Effect of Hot Rolling Finishing Temperature on the Properties of Beryllium Copper Alloy Plates. Rare Metals and Cemented Carbides(1), 128-133.
IEEE [1] HAN Lei, "Study on the Effect of Hot Rolling Finishing Temperature on the Properties of Beryllium Copper Alloy Plates," Rare Metals and Cemented Carbides, no. 1, pp. 128-133, 2026. keywords: {beryllium copper alloy;hot rolling;finishing temperature;mechanical property;microstructure}