Study on New Process of Alkaline Reduction Smelting of Descloizite AITranslate

School of Metallurgy and Environment,Central South University;School of Metallurgy and Environment,Central South University;School of Metallurgy and Environment,Central South University;School of Metallurgy and Environment,Central South University;School of Metallurgy and Environment,Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An alkaline reduction smelting method has been proposed to efficiently extract the valuable metals such as vanadium,lead and zinc from the descloizite ore.Through alkaline reduction smelting process,PbO is reduced to crude lead and deposited at the bottom.ZnO is reduced to zinc and evaporated into flue gas at high temperature,and then collected as ZnO powder from dust collecting system.Vanadium is transformed into soluble vanadate in the smelting slag,and then dissolved into aqueous solution through subsequent leaching process.The main factors affecting smelting and leaching process were investigated.Adding 10% carbon powder and 35% Na_2CO_3 based on descloizite mass and smelting at 1 250 ℃ for 30 min,the crude lead with higher purity than 97% is obtained with 98.6% lead recovery ratio,and the evaporation ratio of zinc reaches 78.9%.After V-containing smelting slag is leached at 95 ℃ for 90 min with 2∶1 solidliquid ratio,vanadium leaching ratio reaches 97.8%.

KeyWords AITranslate

descloizite vanadium lead zinc alkaline reduction smelting leaching

1米玺学.无盐焙烧法提取石煤钒矿中V_2O_5新工艺研究[J].科技创新导报,2012,9(5):19-20. 被引量:4

2蒋馥华.废钒触媒中回收五氧化二钒的新工艺[J].无机盐工业,1989(6):41-43. 被引量:5

3宁华,周晓源,尚德龙,杜海营.石煤提钒焙烧工艺分析[J].有色金属,2010,62(1):80-83. 被引量:17

4孙德功,李健英,孟照芝,祁素芳.从废钒催化剂中回收五氧化二钒[J].河南化工,1996,15(2):30-31. 被引量:4

5李中军,庞锡涛,刘长让.淅川钒矿以NaCl和MnO_2为添加剂的钠化焙烧过程研究[J].稀有金属,1994,18(5):328-333. 被引量:6

6徐盛明,吴延军.碱性直接炼铅法的应用[J].矿产保护与利用,1997(6):31-33. 被引量:25

7宁顺明,马荣骏.我国石煤提钒的技术开发及努力方向[J].矿冶工程,2012,32(5):57-61. 被引量:25

8唐谟堂,唐朝波,陈永明,杨建广,杨声海,何静,欧召.一种很有前途的低碳清洁冶金方法——重金属低温熔盐冶金[J].中国有色冶金,2010,39(4):49-53. 被引量:22

9邓志敢,魏昶,樊刚,李旻廷,李存兄,李兴彬.Extracting vanadium from stone-coal by oxygen pressure acid leaching and solvent extraction[J].中国有色金属学报:英文版,2010,0(S1):118-122. 被引量:15

10叶国华,童雄,路璐.含钒钢渣资源特性及其提钒的研究进展[J].稀有金属,2010,34(5):769-775. 被引量:27

1李建兵.用碱性还原熔炼—水浸工艺从某钒铅矿中提取钒[J].湿法冶金,2020,39(6):490-493. 被引量:1

2张克仑,李博,魏永刚,徐洪傲.钒铅锌矿硫酸浸出提取钒锌[J].过程工程学报,2021,21(11):1297-1303. 被引量:2

1洪颖,郭双华,李雨,田佳蓉.提钒技术研究进展[J].广州化工,2021,49(17):23-25. 被引量:1

2骆晶,温嘉玮,兰春铭,张西华,宁朋歌.微通道中钒的液-液流型和萃取传质动力学研究[J].过程工程学报,2022,22(11):1479-1489.

3艾怡君,李婷婷,夏举佩.氟化铝生产副产物-硅渣酸化过程及其动力学[J].过程工程学报,2023,23(1):115-123.

1П.,ИФ,张登福.用工业五氧化二钒制取钙的钒酸盐[J].四川有色金属,1990(2):19-22.

2魏钦帅,杨斌,李一夫,刘环,戴永年.废铝合金真空蒸馏脱锌的研究[J].真空科学与技术学报,2012,32(5):425-429. 被引量:12

3陈肖虎,陈颖,甘蔓,徐开鑫.沉淀法从拜耳法铝酸钠溶液中分离钒[J].过程工程学报,2010,10(S1):142-145. 被引量:6

4李有奇,柯昌明,李友胜,李楠.金属Zn粉对Al_2O_3-C耐火材料抗氧化性能的影响[J].耐火材料,2006,40(3):200-203. 被引量:6

5张芳,李荣,安胜利,罗果萍.Zn在高炉中热力学行为研究[J].内蒙古科技大学学报,2012,31(3):213-217. 被引量:8

6张延玲,路俊萍,王玉刚,葛西荣辉,郭晓东.FeO-CaO-SiO2-Al2O3渣系中锌及其氯化物的饱和蒸气压测试[J].北京科技大学学报,2008,30(7):717-723.

7熊利芝,陈启元,尹周澜,张平民.真空碳热还原处理低品位氧化铅锌矿热力学分析及实验研究[J].矿冶工程,2009,29(4):64-66. 被引量:9

8范鹤林,陈登福,徐松,龙木军,龙海军.高钙钒比钒渣钠化焙烧熟料浸出条件研究[J].过程工程学报,2013,13(6):958-963. 被引量:14

9张延玲,李士琦,葛西荣辉,路俊萍,郭晓东.Zn在FetO-CaO-SiO2-Al2O3渣系中的挥发行为[J].中国有色金属学报,2008,18(1):163-170. 被引量:1

10朱晓波,张一敏,刘涛.石煤活化焙烧提钒试验及机制研究[J].稀有金属,2013,37(2):283-288. 被引量:11

Basic Information:

DOI:

Chinese Library Classification Number:TF111[冶金工程—冶金物理化学]

Citation Information:

An alkaline reduction smelting method has been proposed to efficiently extract the valuable metals such as vanadium,lead and zinc from the descloizite ore.Through alkaline reduction smelting process,PbO is reduced to crude lead and deposited at the bottom.ZnO is reduced to zinc and evaporated into flue gas at high temperature,and then collected as ZnO powder from dust collecting system.Vanadium is transformed into soluble vanadate in the smelting slag,and then dissolved into aqueous solution through subsequent leaching process.The main factors affecting smelting and leaching process were investigated.Adding 10% carbon powder and 35% Na_2CO_3 based on descloizite mass and smelting at 1 250 ℃ for 30 min,the crude lead with higher purity than 97% is obtained with 98.6% lead recovery ratio,and the evaporation ratio of zinc reaches 78.9%.After V-containing smelting slag is leached at 95 ℃ for 90 min with 2∶1 solidliquid ratio,vanadium leaching ratio reaches 97.8%.

quote

GB/T 7714-2015 [1] HUO Guang-sheng, WU Qian, ZHU Xian-zheng, et al. Study on New Process of Alkaline Reduction Smelting of Descloizite[J]. Rare Metals and Cemented Carbides, 2016(5): 20-25.
MLA [1] HUO Guang-sheng, et al., "Study on New Process of Alkaline Reduction Smelting of Descloizite." Rare Metals and Cemented Carbides, no. 5, 2016, pp. 20-25.
APA [1] HUO Guang-sheng, WU Qian, ZHU Xian-zheng, NI Jie, & LU Xiao-ying. (2016). Study on New Process of Alkaline Reduction Smelting of Descloizite. Rare Metals and Cemented Carbides(5), 20-25.
IEEE [1] HUO Guang-sheng, WU Qian, ZHU Xian-zheng, NI Jie, and LU Xiao-ying, "Study on New Process of Alkaline Reduction Smelting of Descloizite," Rare Metals and Cemented Carbides, no. 5, pp. 20-25, 2016. keywords: {descloizite;vanadium;lead;zinc;alkaline reduction smelting;leaching}