Effects of Nb2O5Content on Structure and Mechanical Properties of Fe/FeAl2O4Cermet AITranslate
Abstract AITranslate
Using Bayan Obo iron concentrate and Al2O3powder as the main raw materials,Fe and FeAl2O4were generated in situ by controllable carbothermal reduction of iron concentrate and sintered at high temperature under normal pressure to prepare Fe/FeAl2O4cermet.The effects of Nb2O5,content on the properties and microstructure of the cermet were discussed.The results show that the two phases in the prepared cermet are uniformly distributed.The addition of Nb2O5can both activate the surface/interface of the cermet particles to facilitate sintering and promote the formation of columnar micro-nano crystals in the ceramic phase.When the content of Nb2O5,is 2%,the mechanical properties can be significantly improved,and the Vickers hardness and bending strength of the cermet under the optimized conditions reach 596 MPa and 132 MPa,respectively.At this time,the fracture of the cermet belongs to ductile fracture.The research can provide a process route for the low-cost preparation of cermet and fully utilize the unique key strategic element niobium resources of Bayan Obo mine.
KeyWords AITranslate
1廖婷婷,李萌崛,陈德平,江万勇,陈嘉鑫.Co,Ni,Ti增韧氧化铝/碳化硅刀具复合材料的制备及性能评价[J].工具技术,2022,56(8):52-55. 被引量:2
2贺涔,江勇,罗思杰.氧化物/不锈钢梯度复合材料的制备及其性能[J].稀有金属材料与工程,2018,47(10):3155-3160. 被引量:1
3达丽梅,周后明,周金虎,刘刚,陈滋鑫,周浩,陈皓月.Al_(2)O_(3)颗粒增韧TiB_(2)-Ti(C_(0.5),N_(0.5))复合陶瓷刀具的力学性能及微观结构[J].材料科学与工程学报,2022,40(5):785-790. 被引量:2
4贾鑫,赵增武,张福顺.烧结温度对Fe/FeAl_2O_4金属陶瓷材料的性能影响[J].功能材料与器件学报,2015,21(5):90-93. 被引量:2
5王闯,张快,严红燕,李运刚.原料质量与FeAl_(2)O_(4)对铁基金属陶瓷力学性能的影响[J].热加工工艺,2021,50(4):12-16. 被引量:1
6李培忠,靳磊,马良,周海滨,王纯,雷新更.Nb和Ta掺杂四方YSZ机械性能及热性能的第一性原理研究[J].稀土,2014,35(6):13-19. 被引量:2
1付国伟,白晓光,吕志义.包钢石灰石型碱性球团试验研究[J].包钢科技,2022,48(5):15-19.
2Wanjia Li,Wangchang Li,Yao Ying,Jing Yu,Jingwu Zheng,Liang Qiao,Juan Li,Shenglei Che.Multifunctional flower-like core-shell Fe/Fe_(4)N@SiO_(2)composites for broadband and high-efficiency ultrathin electromagnetic wave absorber[J].材料科学技术:英文版,2023(1):90-99. 被引量:1
3毛惠东,李芳,覃远航.Fe-Co-N-C氧还原催化剂的制备及性能[J].武汉工程大学学报,2023,45(2):148-155. 被引量:2
4马欣宇,栗鑫,张顺风,韩爱民,陈伟鹏.原位还原制备改性铁精矿载氧体的反应性能[J].粉末冶金工业,2022,32(6):70-76.
5李彩霞,幸世文,李超,赵栖彤.锡添加量对铸态Mg-3Al-0.5SiO_(2)合金显微组织和力学性能的影响[J].机械工程材料,2023,47(3):72-77.
6张颖隆,张明赫,李杰,冯运莉.高熵合金中晶格畸变效应的研究进展[J].热加工工艺,2023,52(4):6-11. 被引量:2
7柴轶凡,樊莹杰,高兴,罗果萍,王艺慈,安胜利.碱度对白云鄂博矿球团矿还原膨胀性能的影响[J].钢铁,2023,58(1):13-21.
8兰晓琳,郑红星,张依帆,赵振,肖和业,王志江,邓鹏飏.常压高温固相反应制备SiC陶瓷粉体的研究进展[J].应用化学,2023,40(4):476-485.
9苗思雨.“双碳”目标下绿色低碳转型对地勘企业盈利能力的影响研究[J].产业创新研究,2023(8):151-153.
10刘稳平.乡村振兴战略背景下公共图书馆精准服务研究[J].传媒论坛,2023,6(6):112-114.
Basic Information:
DOI:
Chinese Library Classification Number:TB33[一般工业技术—材料科学与工程]
Citation Information:
Using Bayan Obo iron concentrate and Al2O3powder as the main raw materials,Fe and FeAl2O4were generated in situ by controllable carbothermal reduction of iron concentrate and sintered at high temperature under normal pressure to prepare Fe/FeAl2O4cermet.The effects of Nb2O5,content on the properties and microstructure of the cermet were discussed.The results show that the two phases in the prepared cermet are uniformly distributed.The addition of Nb2O5can both activate the surface/interface of the cermet particles to facilitate sintering and promote the formation of columnar micro-nano crystals in the ceramic phase.When the content of Nb2O5,is 2%,the mechanical properties can be significantly improved,and the Vickers hardness and bending strength of the cermet under the optimized conditions reach 596 MPa and 132 MPa,respectively.At this time,the fracture of the cermet belongs to ductile fracture.The research can provide a process route for the low-cost preparation of cermet and fully utilize the unique key strategic element niobium resources of Bayan Obo mine.
quote
| GB/T 7714-2015 | [1] ZHANG Fu-shun, HAN Zhi-yuan, ZHOU Ai-hua, et al. Effects of Nb2O5Content on Structure and Mechanical Properties of Fe/FeAl2O4Cermet[J]. Rare Metals and Cemented Carbides, 2023(2): 73-77. |
| MLA | [1] ZHANG Fu-shun, et al., "Effects of Nb2O5Content on Structure and Mechanical Properties of Fe/FeAl2O4Cermet." Rare Metals and Cemented Carbides, no. 2, 2023, pp. 73-77. |
| APA | [1] ZHANG Fu-shun, HAN Zhi-yuan, ZHOU Ai-hua, & JIANG Shi-chen. (2023). Effects of Nb2O5Content on Structure and Mechanical Properties of Fe/FeAl2O4Cermet. Rare Metals and Cemented Carbides(2), 73-77. |
| IEEE | [1] ZHANG Fu-shun, HAN Zhi-yuan, ZHOU Ai-hua, and JIANG Shi-chen, "Effects of Nb2O5Content on Structure and Mechanical Properties of Fe/FeAl2O4Cermet," Rare Metals and Cemented Carbides, no. 2, pp. 73-77, 2023. keywords: {Bayan Obo iron concentrate;FeAlO;cermet;NbO;comprehensive utilization} |