Indium tin oxide (ITO)-free solution-processed transparent electrodes are an essential component for the low-cost fabrication of organic optoelectronic devices. High-performance silver nanowires (AgNWs) ITO-free inverted organic photovoltaics (OPVs) usually require a AgNWs-embedded process. A simple cost-effective roll-to-roll production process of inverted ITO-free OPVs with AgNWs as a bottom transparent electrode requires solution-based thick metal oxides as carrier-selective contacts. In this reported study, we show that a solution-processed antimony-doped tin oxide (ATO)/polyethylenimine (PEI) electron-selective contact incorporated on the top of non-embedded AgNWs provides a high-performance ITO-free bottom electrode for non-fullerene acceptor (NFA) inverted OPVs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01187
Chinese Library Classification Number:
Citation Information:
Indium tin oxide (ITO)-free solution-processed transparent electrodes are an essential component for the low-cost fabrication of organic optoelectronic devices. High-performance silver nanowires (AgNWs) ITO-free inverted organic photovoltaics (OPVs) usually require a AgNWs-embedded process. A simple cost-effective roll-to-roll production process of inverted ITO-free OPVs with AgNWs as a bottom transparent electrode requires solution-based thick metal oxides as carrier-selective contacts. In this reported study, we show that a solution-processed antimony-doped tin oxide (ATO)/polyethylenimine (PEI) electron-selective contact incorporated on the top of non-embedded AgNWs provides a high-performance ITO-free bottom electrode for non-fullerene acceptor (NFA) inverted OPVs.
quote
| GB/T 7714-2015 | [1] Efthymios Georgiou, Apostolos Ioakeimidis, Ioanna Antoniou, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01187. |
| MLA | [1] Efthymios Georgiou, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01187. |
| APA | [1] Efthymios Georgiou, Apostolos Ioakeimidis, Ioanna Antoniou, Ioannis T. Papadas, Alina Hauser, Michael Rossier, Flavio Linardi, & Stelios A. Choulis. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01187 |
| IEEE | [1] Efthymios Georgiou, Apostolos Ioakeimidis, Ioanna Antoniou, Ioannis T. Papadas, Alina Hauser, Michael Rossier, Flavio Linardi, and Stelios A. Choulis, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01187. keywords: {ITOfree organic photovoltaics silver nanowires doped metal oxides carrierselective contact electrodes inverted organic solar cells printed electronics} |