Study on Synthesis of Calix[8]arene Derivatives and their Performance for La and Ce Extraction Separation AITranslate

Hunan Institute of Technology Institute of Chemistry and Chemical Engineering;Hunan Institute of Technology Institute of Chemistry and Chemical Engineering;Hunan Institute of Technology Institute of Chemistry and Chemical Engineering
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A series of calix]-8]arene phosphate derivatives with high extraction efficiency to light rare earth ions and a certain selectivity were synthesized by one step of substitution reaction. The results show that the extraction ratio of La and Ce light rare earth is up to 98% with the calix[8]arene phosphate derivatives,10% higher than that with calix[8-]arene. Under the same conditions and with the calix[8]arene phosphate derivatives,La extraction ratio is 6 % higher than Ce extraction ratio. Efficient extraction separa- tion of La and Ce ions can be achieved by multi-stage centrifugal extraction fractionation.

KeyWords AITranslate

calix[-8]arene phosphate derivative one-step synthesis lanthanum cerium extraction separation

1郭耘,卢冠忠.稀土催化材料的应用及研究进展[J].中国稀土学报,2007,25(1):1-15. 被引量:53

2武芸,曹端林,李永祥.对叔丁基杯[6]芳烃合成[J].应用化工,2006,35(11):871-872. 被引量:5

1杨歆,梁恩湘,易健民.杯[8]芳烃磷酸酯萃取分离镧铈混合离子的研究[J].稀有金属与硬质合金,2019,47(4):7-12.

1胡灵卫,理记涛.氧化锌/石墨烯复合材料的制备、表征及发光性质研究[J].周口师范学院学报,2017,34(2):56-58.

2柯怡达.童真之趣[J].汽车与配件,2017,0(31):50-57.

3张利珍,谭秀民,张秀峰,张永兴,李琦.以t-BAMBP+磺化煤油萃取体系萃取分离低浓度的铷[J].无机盐工业,2017,49(11):37-40. 被引量:2

4李佳,黄永庆.磷酸三丁酯萃取分离磷-电感耦合等离子体原子发射光谱法测定高纯黄磷中铁锌硅铝[J].冶金分析,2017,37(11):52-58. 被引量:1

5周佳,方秋生,余治宇,宋智彬.多羟基1,2-二取代苯并咪唑的选择性合成和抗氧化性质研究[J].江西师范大学学报:自然科学版,2017,41(4):424-427. 被引量:1

6王彩英,王士智,李平.稀土萃取分离工艺的改进与废水循环利用研究[J].稀有金属与硬质合金,2017,45(5):7-10. 被引量:5

7张洪菡,张善鹤,李春义.多级孔ZSM-5分子筛的一步合成及反应性能[J].石化技术与应用,2017,35(6):429-433. 被引量:1

8陈润康,莫平菁,黄安旗,李素,张敏,张燕,程发良.基于雪花形状的金纳米结构的抗坏血酸传感器的研究[J].广东化工,2017,44(21):35-37.

9郑坤,赵娇娇,陈莹,王春鹏,储富祥.高力学强度羟乙基纤维素/聚丙烯酰胺复合水凝胶的制备[J].高分子材料科学与工程,2017,33(11):6-11. 被引量:5

10苏帅,徐清,范冬梅,翟春阳.介孔碳负载Ce-TiO_2的制备及其光催化降解亚甲蓝性能[J].人工晶体学报,2017,46(8):1580-1586. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O625.34[理学—有机化学]

Citation Information:

A series of calix]-8]arene phosphate derivatives with high extraction efficiency to light rare earth ions and a certain selectivity were synthesized by one step of substitution reaction. The results show that the extraction ratio of La and Ce light rare earth is up to 98% with the calix[8]arene phosphate derivatives,10% higher than that with calix[8-]arene. Under the same conditions and with the calix[8]arene phosphate derivatives,La extraction ratio is 6 % higher than Ce extraction ratio. Efficient extraction separa- tion of La and Ce ions can be achieved by multi-stage centrifugal extraction fractionation.

quote

GB/T 7714-2015 [1] LIU Xiang-zhi, LIANG En-xiang, YI Jian-min. Study on Synthesis of Calix[8]arene Derivatives and their Performance for La and Ce Extraction Separation[J]. Rare Metals and Cemented Carbides, 2017(5): 37-41.
MLA [1] LIU Xiang-zhi, et al., "Study on Synthesis of Calix[8]arene Derivatives and their Performance for La and Ce Extraction Separation." Rare Metals and Cemented Carbides, no. 5, 2017, pp. 37-41.
APA [1] LIU Xiang-zhi, LIANG En-xiang, & YI Jian-min. (2017). Study on Synthesis of Calix[8]arene Derivatives and their Performance for La and Ce Extraction Separation. Rare Metals and Cemented Carbides(5), 37-41.
IEEE [1] LIU Xiang-zhi, LIANG En-xiang, and YI Jian-min, "Study on Synthesis of Calix[8]arene Derivatives and their Performance for La and Ce Extraction Separation," Rare Metals and Cemented Carbides, no. 5, pp. 37-41, 2017. keywords: {calix[-8]arene phosphate derivative;one-step synthesis;lanthanum;cerium;extraction separation}