daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tuning the Conductivity, Morphology, and Capacitance with Enhanced Antibacterial Properties of Polypyrrole by Acriflavine Hydrochloride AITranslate

Institute of Macromolecular Chemistry;Institute of Macromolecular Chemistry; Tomas Bata University in Zlín;Institute of Macromolecular Chemistry;Institute of Macromolecular Chemistry; Tomas Bata University in Zlín; Tomas Bata University in Zlín;Institute of Macromolecular Chemistry
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this study, a simple one-step preparation of polypyrrole (PPy) assisted by an organic dye, acriflavine hydrochloride (AF), was investigated. The presence of a dye resulted in the development of PPy nanofibers with the conductivity enhanced up to 14 S cm–1. The structural analysis by Fourier-transform infrared and Raman spectroscopies confirmed the interaction of the AF with PPy. As far as the electrochemical activity of PPy is concerned, the gravimetric capacitance increased up to 85 F g–1 with the help of a AF. Additionally, a substantial improvement in the antibacterial activity against Staphylococcus aureus and Escherichia coli bacteria for all the PPy-containing organic dye was achieved. The conductivity, morphology, capacitance, and remarkable antibacterial properties of PPy tuned by an organic dye enable applications wherever the electroconductivity and antibacterial activity should meet requirements, for example, wound healing, electrochemical sensors, bioactuators, or even regenerative medicine.

KeyWords AITranslate

acriflavine hydrochloride polypyrrole nanofibers conductivity capacitance antibacterial activity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00775

Chinese Library Classification Number:

Citation Information:

In this study, a simple one-step preparation of polypyrrole (PPy) assisted by an organic dye, acriflavine hydrochloride (AF), was investigated. The presence of a dye resulted in the development of PPy nanofibers with the conductivity enhanced up to 14 S cm–1. The structural analysis by Fourier-transform infrared and Raman spectroscopies confirmed the interaction of the AF with PPy. As far as the electrochemical activity of PPy is concerned, the gravimetric capacitance increased up to 85 F g–1 with the help of a AF. Additionally, a substantial improvement in the antibacterial activity against Staphylococcus aureus and Escherichia coli bacteria for all the PPy-containing organic dye was achieved. The conductivity, morphology, capacitance, and remarkable antibacterial properties of PPy tuned by an organic dye enable applications wherever the electroconductivity and antibacterial activity should meet requirements, for example, wound healing, electrochemical sensors, bioactuators, or even regenerative medicine.

quote

GB/T 7714-2015 [1] Sonal Gupta, Udit Acharya, Hana Pištěková, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00775.
MLA [1] Sonal Gupta, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00775.
APA [1] Sonal Gupta, Udit Acharya, Hana Pištěková, Oumayma Taboubi, Zuzana Morávková, Martina Kašparová, Petr Humpolíček, & Patrycja Bober. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00775
IEEE [1] Sonal Gupta, Udit Acharya, Hana Pištěková, Oumayma Taboubi, Zuzana Morávková, Martina Kašparová, Petr Humpolíček, and Patrycja Bober, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00775. keywords: {acriflavine hydrochloride;polypyrrole;nanofibers;conductivity;capacitance;antibacterial activity}