Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000;Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000;Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000;Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000;Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000;Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000;Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000;Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000;Jiangxi Provincial Key Laboratory of Low-carbon Processing and Utilization of Strategic Metal Mineral Resources,Jiangxi University of Science and Technology,Ganzhou 341000
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Developing efficient non-lime inhibitors for iron sulfide minerals is a crucial research direction in the field of sulfide ores flotation.This study investigated the flotation characteristics of monoclinic pyrrhotite and examined the effects of three oxidants on its flotation behavior.The interaction mechanism between potassium permanganate oxidant and monoclinic pyrrhotite was elucidated using flotation kinetics,adsorption tests,and X-ray photoelectron spectroscopy(XPS).Flotation experiments demonstrated that the addition of a small amount of potassium permanganate exhibited a superior inhibitory effect on monoclinic pyrrhotite across a wide pH range compared to the high-alkali lime system,reducing the flotation recovery to as low as 6.23%.XPS analysis revealed that after treatment with potassium permanganate,the binding energies of multiple characteristic peaks for Fe 2p and S 2p on the monoclinic pyrrhotite surface exhibited significant shifts.Additionally,the relative sulfur content and the sulfurto-iron ratio decreased markedly.It was inferred that surface oxidation led to the formation of abundant hydrophilic products,such as Fe(OH)3,SO42-,and ferrous sulfate hydrates.These products substantially weakened the adsorption of collector,resulting in a significant reduction in both the flotation rate and the recovery of monoclinic pyrrhotite.

KeyWords AITranslate

monoclinic pyrrhotite surface oxidation inhibitors flotation behavior flotation kinetics
No data

Basic Information:

DOI:

Chinese Library Classification Number:TD951[矿业工程—选矿];TD923

Citation Information:

Developing efficient non-lime inhibitors for iron sulfide minerals is a crucial research direction in the field of sulfide ores flotation.This study investigated the flotation characteristics of monoclinic pyrrhotite and examined the effects of three oxidants on its flotation behavior.The interaction mechanism between potassium permanganate oxidant and monoclinic pyrrhotite was elucidated using flotation kinetics,adsorption tests,and X-ray photoelectron spectroscopy(XPS).Flotation experiments demonstrated that the addition of a small amount of potassium permanganate exhibited a superior inhibitory effect on monoclinic pyrrhotite across a wide pH range compared to the high-alkali lime system,reducing the flotation recovery to as low as 6.23%.XPS analysis revealed that after treatment with potassium permanganate,the binding energies of multiple characteristic peaks for Fe 2p and S 2p on the monoclinic pyrrhotite surface exhibited significant shifts.Additionally,the relative sulfur content and the sulfurto-iron ratio decreased markedly.It was inferred that surface oxidation led to the formation of abundant hydrophilic products,such as Fe(OH)3,SO42-,and ferrous sulfate hydrates.These products substantially weakened the adsorption of collector,resulting in a significant reduction in both the flotation rate and the recovery of monoclinic pyrrhotite.

quote

GB/T 7714-2015 [1] LI Zetao, CHEN Jie, TANG Honghu, et al. Influence mechanism of potassium permanganate oxidation on the flotation behavior of monoclinic pyrrhotite[J]. Nonferrous Metals Science and Engineering, 2026(2): 310-317.
MLA [1] LI Zetao, et al., "Influence mechanism of potassium permanganate oxidation on the flotation behavior of monoclinic pyrrhotite." Nonferrous Metals Science and Engineering, no. 2, 2026, pp. 310-317.
APA [1] LI Zetao, CHEN Jie, TANG Honghu, ZHOU Shaobing, WU Qiming, CHEN Jinghe, ZOU Laichang, YAN Huashan, & QIU Tingsheng. (2026). Influence mechanism of potassium permanganate oxidation on the flotation behavior of monoclinic pyrrhotite. Nonferrous Metals Science and Engineering(2), 310-317.
IEEE [1] LI Zetao, CHEN Jie, TANG Honghu, ZHOU Shaobing, WU Qiming, CHEN Jinghe, ZOU Laichang, YAN Huashan, and QIU Tingsheng, "Influence mechanism of potassium permanganate oxidation on the flotation behavior of monoclinic pyrrhotite," Nonferrous Metals Science and Engineering, no. 2, pp. 310-317, 2026. keywords: {monoclinic pyrrhotite;surface oxidation;inhibitors;flotation behavior;flotation kinetics}