Abstract AITranslate

<Abstrcat>In the paper is reviewed the development status of cemented carbide coating technology and products of in Kennametal Inc.since 1979.

KeyWords AITranslate

Kennametal Inc cutting tool coating technology nanolayered coating development status

1Brookes K J A.Materials research at Kennametal Inc[J].Metal Powder Report,1983,38(7):378.

2North Bernard.The past,present,and future of cemented carbides-A technical overview[A].International Tungsten Industry Association.9th International Tungsten Symposium[C].Pittsburgh:Kennametal Inc,2002.96.

3Kennametal Inc.Nanolayered coated cutting tool and method for making the same[P].WO Pat:03/078689 A1,2003-09-25.

4Brookes K J A.World Directory and Handbook of Hardmetals and Hard Materials(Sixth edition)[M].United Kingdom:International Carbide Data,1996.

5Kennametal Inc.KENNAMETAL 2002 Cutting Tools[M].Pittsburgh:Kennametal Inc,2002.

1余东海,王成勇,张凤林.刀具涂层材料研究进展[J].工具技术,2007,41(6):25-32. 被引量:36

2陈勇志,占志泽,曾铁初.硬质合金涂层技术及其进展[J].东莞理工学院学报,2012,19(3):94-98. 被引量:3

3商成超,仰磊.汽车发动机加工刀具涂层技术的应用[J].工具技术,2020,54(8):73-74. 被引量:1

1庆振华,谢峰,张崇高,杨海东,周之江.基于仿生学的刀具研究初探[J].工具技术,2008,42(9):3-6. 被引量:9

2罗来马,俞佳,刘少光,郦剑.低合金高速钢的物理气相沉积技术应用与发展[J].金属热处理,2008,33(11):13-16. 被引量:1

3赵玉玲,丰平,张晓明,熊惟皓.涂层硬质合金结构及材料的研究进展[J].中国陶瓷,2009(4):3-8. 被引量:2

4陈颢,羊建高,王宝健,刘海浪.硬质合金刀具涂层技术现状及展望[J].硬质合金,2009,26(1):54-58. 被引量:30

5赵玉玲,丰平,张晓明,熊惟皓.涂层硬质合金的最新研究进展[J].材料开发与应用,2009,24(2):94-101. 被引量:4

6王焱,王文理.先进刀具技术与航空零件切削加工[J].航空制造技术,2009,0(23):36-42. 被引量:9

7谭敦强,刘阳,龙建,郭锐,陆德平,尹桦.涂层硬质合金的回收过程中涂层剥离技术发展现状[J].粉末冶金工业,2011,21(6):54-59. 被引量:3

8徐涛.硬质合金高端产品及新材料发展趋势分析[J].硬质合金,2011,28(6):395-402. 被引量:40

9韩振威,林有希.TiAlSiN涂层刀具研究新进展[J].工具技术,2012,46(2):3-7. 被引量:7

10邱家稳,赵栋才.电弧离子镀技术及其在硬质薄膜方面的应用[J].表面技术,2012,41(2):93-100. 被引量:19

1StaffanSoderberg,佘建芳.金属切削刀具涂层技术的发展[J].国外难熔金属与硬质材料,2002,18(2):41-48. 被引量:2

2李洪林,李波,胡恒宁,高见.刀具涂层技术的最新发展状况[J].工具技术,2010,44(4):3-6. 被引量:18

3开发cBN涂层技术难点[J].超硬材料工程,2010(3):15-15.

4姚英学,张宏志,袁哲俊,黄树涛.金刚石薄膜涂层刀具及其应用[J].高技术通讯,1996,6(1):54-58. 被引量:7

5赵海波.国内外切削刀具涂层技术发展综述[J].工具技术,2002,36(2):3-7. 被引量:51

6袁家栋.涂层技术与现代切削刀具的互动发展[J].金属热处理,2007,32(8):1-4. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG711[金属学及工艺—刀具与模具]

Citation Information:

<Abstrcat>In the paper is reviewed the development status of cemented carbide coating technology and products of in Kennametal Inc.since 1979.

quote

GB/T 7714-2015 [1] SHE Jian-fang. Development of Coating Technology for Cutting Tools in Kennametal Inc[J]. Rare Metals and Cemented Carbides, 2005(2): 59-62.
MLA [1] SHE Jian-fang. "Development of Coating Technology for Cutting Tools in Kennametal Inc." Rare Metals and Cemented Carbides, no. 2, 2005, pp. 59-62.
APA [1] SHE Jian-fang. (2005). Development of Coating Technology for Cutting Tools in Kennametal Inc. Rare Metals and Cemented Carbides(2), 59-62.
IEEE [1] SHE Jian-fang, "Development of Coating Technology for Cutting Tools in Kennametal Inc," Rare Metals and Cemented Carbides, no. 2, pp. 59-62, 2005. keywords: {Kennametal Inc;cutting tool;coating technology;nanolayered coating;development status}