daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tuning the Properties of Nanocomposites by Trapping Them in Deep Metastable States AITranslate

Oak Ridge National Laboratory; Oak Ridge National Laboratory; Oak Ridge National Laboratory; Université de Montpellier; University of Tennessee; University of Tennessee; Oak Ridge National Laboratory; University of Tennessee; Oak Ridge National Laboratory; Oak Ridge National Laboratory; Argonne National Laboratory; University of Tennessee
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The interfacial region formed in a polymer matrix around nanoparticles (NPs) controls many macroscopic properties of polymer nanocomposites (PNCs). However, understanding the factors controlling the structure and properties of the interfacial region remains a challenge. We demonstrated that the initial trapping of polymer chains at surfaces of NPs in solution strongly affects the macroscopic properties of PNCs. The most surprising result is that the differences in properties of PNCs persist even after an extremely long thermal annealing time. We ascribe the observed changes to the formation of an interfacial layer that is trapped in a deep metastable state already in solution. Furthermore, the presented analysis suggests that the PNC equilibration time is defined by the chain desorption time that can be extremely long and, in some cases, even not accessible on a reasonable experimental time scale. These results highlight the importance of polymer solution concentrations on the formation of an interfacial layer and the macroscopic properties of PNCs.

KeyWords AITranslate

Polymer nanocomposites photon correlation spectroscopy interfacial layer model Brillouin light scattering SCFT calculations
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01623

Chinese Library Classification Number:

Citation Information:

The interfacial region formed in a polymer matrix around nanoparticles (NPs) controls many macroscopic properties of polymer nanocomposites (PNCs). However, understanding the factors controlling the structure and properties of the interfacial region remains a challenge. We demonstrated that the initial trapping of polymer chains at surfaces of NPs in solution strongly affects the macroscopic properties of PNCs. The most surprising result is that the differences in properties of PNCs persist even after an extremely long thermal annealing time. We ascribe the observed changes to the formation of an interfacial layer that is trapped in a deep metastable state already in solution. Furthermore, the presented analysis suggests that the PNC equilibration time is defined by the chain desorption time that can be extremely long and, in some cases, even not accessible on a reasonable experimental time scale. These results highlight the importance of polymer solution concentrations on the formation of an interfacial layer and the macroscopic properties of PNCs.

quote

GB/T 7714-2015 [1] Zhengping Zhou, Vera Bocharova, Rajeev Kumar, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01623.
MLA [1] Zhengping Zhou, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01623.
APA [1] Zhengping Zhou, Vera Bocharova, Rajeev Kumar, AnneCaroline Genix, Bobby Carroll, Subarna Samanta, Ivan Popov, Amanda YoungGonzales, Alexander Kisliuk, Seung Pyo Jeong, Jan Ilavsky, & Alexei P. Sokolov. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01623
IEEE [1] Zhengping Zhou, Vera Bocharova, Rajeev Kumar, AnneCaroline Genix, Bobby Carroll, Subarna Samanta, Ivan Popov, Amanda YoungGonzales, Alexander Kisliuk, Seung Pyo Jeong, Jan Ilavsky, and Alexei P. Sokolov, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01623. keywords: {Polymer nanocomposites;photon correlation spectroscopy;interfacial layer model;Brillouin light scattering;SCFT calculations}