daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Freestanding Membranes for Unique Functionality in Electronics Freestanding Membranes for Unique Functionality in Electronics AITranslate

Sungkyunkwan University; Washington University in St. Louis; Washington University in St. Louis; Washington University in St. Louis; Washington University in St. Louis; Washington University in St. Louis; University of Science and Technology; Sungkyunkwan University; Washington University in St. Louis
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Epitaxy of single-crystalline materials laid the foundation for numerous electronics as a core technology. Nevertheless, because the single-crystalline epilayers are covalently bonded to substrates, only limited applications were explored. The recent development of layer transfer techniques has suggested another way involving the production of freestanding membranes that are free from substrates. In this review, we comprehensively catalog recent advances for freestanding-membrane-based electronics from transistors and memory storage to sensors and energy harvesters. We highlight their unique advantages, including flexibility, unique physical coupling, heterointegrability, and cost-effectiveness, and summarize their challenges and perspectives.

KeyWords AITranslate

freestanding membranes epitaxy thin films twodimensional materials heterointegration electronics
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01411

Chinese Library Classification Number:

Citation Information:

Epitaxy of single-crystalline materials laid the foundation for numerous electronics as a core technology. Nevertheless, because the single-crystalline epilayers are covalently bonded to substrates, only limited applications were explored. The recent development of layer transfer techniques has suggested another way involving the production of freestanding membranes that are free from substrates. In this review, we comprehensively catalog recent advances for freestanding-membrane-based electronics from transistors and memory storage to sensors and energy harvesters. We highlight their unique advantages, including flexibility, unique physical coupling, heterointegrability, and cost-effectiveness, and summarize their challenges and perspectives.

quote

GB/T 7714-2015 [1] Sangmoon Han, Yuan Meng, Zhihao Xu, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01411.
MLA [1] Sangmoon Han, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01411.
APA [1] Sangmoon Han, Yuan Meng, Zhihao Xu, Justin S. Kim, Yimeng Li, IlPyo Roh, Hyojung Ahn, DongHwan Kim, & SangHoon Bae. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01411
IEEE [1] Sangmoon Han, Yuan Meng, Zhihao Xu, Justin S. Kim, Yimeng Li, IlPyo Roh, Hyojung Ahn, DongHwan Kim, and SangHoon Bae, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01411. keywords: {freestanding membranes epitaxy thin films twodimensional materials heterointegration electronics}